Alloy Digest (1979) 28 (9): Al-157.
Published: 01 September 1979
... ALUMINUM 5254 is an aluminum-magnesium-chromium wrought alloy of the non-heat-treatable type; however, it can be hardened and strengthened by cold working. It is relatively strong and has excellent resistance to general corrosion and stress-corrosion cracking. Its applications include hydrogen...
Journal Articles
Alloy Digest (2002) 51 (7): Al-379.
Published: 01 July 2002
... joinability physical properties shear strength thermal properties Chemical Composition, wt Silicon + iron 0.45 max Copper 0.05 max Manganese 0.01 max Magnesium 3.1 3.9 Chromium 0.15 0.35 Zinc 0.20 max Titanium 0.05 0.15 Beryllium 0.0008 max Others, each 0.05 max Others, total 0.15 max Aluminum bal...
Journal Articles
Alloy Digest (1963) 12 (8): Al-128.
Published: 01 August 1963
... Alcan B51S is a medium strength, heat treatable aluminum structural alloy. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining...