Alloy Digest (1982) 31 (2): Al-236.
Published: 01 February 1982
... ALUMINUM 514.0 is a non-heat-treatable alloy containing nominally 4% magnesium. It has relatively low strength and hardness. It is characterized by excellent weldability and excellent resistance to corrosion. Aluminum 514.0 is recommended for food-processing equipment and marine applications...
Journal Articles
Alloy Digest (1987) 36 (4): Al-280.
Published: 01 April 1987
... and pitting corrosion. It is highly resistant to seawater and high-octane gasoline fuels. It resists mild alkalies or salt spray. Specification Equivalents: ALUMINUM 51410. AA 514.0. ASTM B 2q514.0). Federal QQ-A-601(514.0) Military MILK-I 1866(214). SAE: J452(320) and J453(320). General Characteristics: UNS...