1-16 of 16 Search Results for

ALUMINUM 5083

Sort by
Journal Articles
Alloy Digest (1978) 27 (10): Al-33.
Published: 01 October 1978
... ALUMINUM 5083 is a non-heat-treatable wrought aluminum alloy possessing high strength, excellent welding characteristics and excellent resistance to corrosion. Among its many applications are structural towers, mobile cranes and chemical storage tanks. This datasheet provides information...
Journal Articles
Alloy Digest (2023) 72 (1): Al-493.
Published: 01 January 2023
... Austral Wright 5083 is a wrought, non-heat-treatable, aluminum-magnesium-manganese-chromium alloy (5xxx series). It has the highest strength of the non-heat-treatable alloys but is not recommended for use at temperatures in excess of 65 °C (150 °F). It is among the most widely used aluminum alloys...
Journal Articles
Alloy Digest (1959) 8 (11): Al-85.
Published: 01 November 1959
.... 1477jNP5j6 Plate B.S. 1490,QMSM. castings u. s. Aluminum 5083 (approx.) Aluminum 5456 (approx.) General Characteristics: This alloy is eminently suitable for applications where a high standard of corrosion resistance is necessary with a good combination of rigidiy and high shock resistance. It requires...
Journal Articles
Alloy Digest (1966) 15 (4): Al-154.
Published: 01 April 1966
...-gas tungsten-arc (TIG) and by the metal- arc-inert-gas (MIG) process, using a weld filler alloy of Aluminum X5039 or 5183 rod. It has considerably better weld screngch and ductility than Aluminum 5083. Ic is readily welded over a wide range of thicknesses with no decrease in weld ductility. IC also...
Journal Articles
Alloy Digest (2020) 69 (9): Al-468.
Published: 01 September 2020
... joinability machinability physical properties tensile properties workability UNS A95083 ATLAS 5083 (Non-Heat-Treatable, Al-4.5Mg-0.7Mn-0.15Cr Alloy) Filing Code: Al-468 Aluminum :: September 2020 :: :: :: ::Materials Park, Ohio 44073-0002 440.338.5151 Fax 440.338.4634 www.asminternational.org...
Journal Articles
Alloy Digest (2003) 52 (1): Al-384.
Published: 01 January 2003
... Alcotec Weld filler wire 5183 is a non-heat-treatable aluminum welding wire whose principal alloying elements are magnesium, manganese, and chromium. It is similar to the European wire AlMg4.5Mn. This datasheet provides information on composition, physical properties, and tensile properties...
Journal Articles
Alloy Digest (2004) 53 (6): Al-390.
Published: 01 June 2004
... in. 76 Hardness, as supplied, HB 75 Young s modulus, GPa (106 psi) 73.8 (10.7) See also Table 1 and Fig. 1. General Characteristics: Giantal is a highly developed form of 5083-O, the alloy used in fabricating the first generation of aluminum tools. Giantal is dis- tinguished by significantly low internal...
Journal Articles
Alloy Digest (1989) 38 (5): Al-296.
Published: 01 May 1989
... IncoMAP alloy Al-9052 is a high-strength, corrosion resistant aluminum alloy made by the mechanical alloying process. It is dispersion strengthened by oxides and carbides. Its density is 5% less than age hardenable aluminum alloys of comparable strength. This datasheet provides information...
Journal Articles
Alloy Digest (2002) 51 (4): Al-376.
Published: 01 April 2002
... Wire Corporation. Producer or Source: AlcoTec Wire Corporation Copyright © ASM International® 2002 2002 ASM International ALCOTEC WELD WIRE 5356 chemical composition joinability physical properties shear strength tensile properties wires wrought aluminum alloys thermal properties...
Journal Articles
Alloy Digest (2022) 71 (7): Al-488.
Published: 01 July 2022
... Atlas 6063 is a wrought, heat-treatable, aluminum-magnesium-silicon extrusion alloy (6xxx series) that offers good mechanical properties. It responds well to polishing, chemical brightening, anodizing, and dyeing. This datasheet provides information on composition, physical properties, elasticity...
Journal Articles
Alloy Digest (2004) 53 (5): Al-387.
Published: 01 May 2004
... for mold applications are based on the 2xxx series aluminum alloys. This alloy is similar to 2219. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on high temperature performance as well as joining. Filing...
Journal Articles
Alloy Digest (1966) 15 (10): Al-159.
Published: 01 October 1966
... Aluminum 7002 is a heat treatable, weldable, high strength aluminum alloy recommended for space equipment and cryogenic applications. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive and shear strength as well...
Journal Articles
Alloy Digest (2003) 52 (12): Al-275.
Published: 01 December 2003
... manufacturer. Corrosion Resistance: This alloy has excellent corrosion resistance. It has resistance to exfoliation corrosion and stress-corrosion cracking. Stress- corrosion cracking can be an issue with alloys containing more than 3% Mg such as 5086 and 5083. Aluminum can be subject to galvanic action when...
Journal Articles
Alloy Digest (1979) 28 (4): Al-234.
Published: 01 April 1979
.... It is also com- parable to that of the standard wrought aluminum alloys used for armor plate, 5083 and 7039. The proprietor can provide details on these ballistic tests. Specification Equivalents: The following military and aerospace procurement specifications include A201 alloy: MIL-A-21180 and MIL-HDBKJ...
Journal Articles
Alloy Digest (1966) 15 (4): Ti-47.
Published: 01 April 1966
... HYLITE 20 is a titanium-aluminum-tin alloy with properties of medium tensile strength, good weldability and non-embrittlement under service conditions. It is recommended for aircraft and missile components. This datasheet provides information on composition, physical properties, elasticity...
Journal Articles
Alloy Digest (1988) 37 (7): Al-282.
Published: 01 July 1988
... Alcoa Aluminum Alloy 6013 is a high-strength Al-Mg-Si-Cu alloy. It is available in five tempers. It is crossing many market areas of applications in aerospace, defense, automotive and general structural use. This datasheet provides information on composition, physical properties, elasticity...