1-3 of 3 Search Results for

ALUMINUM 384.0

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Alloy Digest (1975) 24 (10): Al-218.
Published: 01 October 1975
... ALUMINUM 384.0 is a general-purpose alloy for making intricate die castings. It has good castability and foundry characteristics, good machinability and good strength. It is an excellent alloy for large thin-walled castings, and is suitable for castings requiring pressure tightness. This datasheet...
Journal Articles
Alloy Digest (1991) 40 (2): Al-312.
Published: 01 February 1991
.... Filing Code: Al-312. Producer or source: Various aluminum companies. Producer or Source: Various aluminum companies Copyright © ASM International® 1996 1996 ASM International cast aluminum alloys castability chemical composition corrosion-resistant alloys elasticity fatigue properties...
Journal Articles
Alloy Digest (1977) 26 (5): Al-226.
Published: 01 May 1977
... as casting, heat treating, machining, and joining. Filing Code: Al-226. Producer or source: Federated Metals Corporation, ASARCO Inc.. Producer or Source: Federated Metals Corporation, ASARCO Inc. Copyright © ASM International® 1996 1996 ASM International cast aluminum alloys castability...