Journal Articles
Alloy Digest (1976) 25 (5): Al-223.
Published: 01 May 1976
... ALUMINUM 356.0 is an aluminum casting alloy that normally is used only when heat-treated (aged) strengths are required. It is recommended for high strength, pressure-tight castings, intricate shapes and good resistance to corrosion. Its many applications include gear cases, instrument housings...
Journal Articles
Alloy Digest (1992) 41 (7): Al-323.
Published: 01 July 1992
... Alloys R-A356.0, ER4010 and R4010 include aluminum-silicon-magnesium Almigweld and Altigweld filler wires with low iron content to weld alloys 356.0 (Alloy Digest Al-223, May 1976) and A356.0 (Alloy Digest Al-258, June 1985). This datasheet provides information on composition and physical...
Journal Articles
Alloy Digest (2023) 72 (6): Al-499.
Published: 01 June 2023
...)(a) 22.6 (39)(a) Typical values. (a) For alloy A356.0 sand castings in the T6 temper. Source: 356.0 and A356.0: Al-Si-Mg High-Strength Casting Alloys, Properties and Selection of Aluminum Alloys, Volume 2B, ASM Handbook, ASM International, 2019, p 548 httpsdoi.org/10.31399/asm.ad.al0499 ISSN: 002-614X...
Journal Articles
Alloy Digest (2022) 71 (3): Al-486.
Published: 01 March 2022
... Rio Tinto 355.2 is a heat-treatable, aluminum-silicon-copper-magnesium casting alloy (3xx.x series). It is available in the form of ingots for remelting, for the production of sand and permanent mold castings. It is a high-strength alloy with many desirable characteristics. The presence of copper...
Journal Articles
Alloy Digest (2023) 72 (5): Al-498.
Published: 01 May 2023
...) 2685 (0.097) 21.5 (11.9) 22.5 (12.5) 23.5 (13.1) 151 (87.3)(a) 963 (0.230) 0.0442 (26.6)(a) 22.6 (39)(a) Typical values. (a) For alloy 356.0 sand castings in the T6 temper. Source: 356.0 and A356.0: Al-Si-Mg High-Strength Casting Alloys, Properties and Selection of Aluminum Alloys, Volume 2B, ASM...
Journal Articles
Alloy Digest (1974) 23 (10): Al-209.
Published: 01 October 1974
... by standard corrosion tests. It has excellent resistance to most forms of corrosion; it is somewhat better than Aluminum 355 in this respect. Chemical conversion coatings give further protection. Specification Equivalents: Sand Castings: AA No. 356.0; ASTM B 26, 356.0 (SG70A); SAP 356.0 (323); Federal QQ...
Journal Articles
Alloy Digest (1970) 19 (10): Al-200.
Published: 01 October 1970
... is comparable with alloy 295.0 i.e. less resistant than alloy 356.0. Specification Equivalents: At present there are no government or technical society specifications for alloy 224.0. General Characteristics: ALUMINUM Alloy 224.0, a variation of wrought alloy 2219, was developed for the production of sand...
Journal Articles
Alloy Digest (1979) 28 (4): Al-234.
Published: 01 April 1979
.... The T-7 condition meets all of the stress- corrosion standards established for high-strength aluminum alloys Ballistic Properties: In actual firing tests, the ballistic weight merit rating of Aluminum A201.0-T7 is superior to two other high-strength aluminum casting alloys, 224GT7 and 356.0-T61...
Journal Articles
Alloy Digest (2022) 71 (10): Al-490.
Published: 01 October 2022
... Rio Tinto C355.2 is a heat-treatable, aluminum-silicon-copper-magnesium casting alloy (3xx.x series). It is available in the form of ingots for remelting, to be used for the production of sand and permanent mold castings. Alloy C355.0 is a higher purity, low iron version of alloy 355.0. Both...
Journal Articles
Alloy Digest (1995) 44 (8): Al-338.
Published: 01 August 1995
... ALUMINUM ALLOY 771.0 can be sand or permanent mold cast and naturally aged at room temperature. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes information on casting, heat treating, machining, joining, and surface...
Journal Articles
Alloy Digest (2021) 70 (4): Al-475.
Published: 01 April 2021
... AB-Al Si7Mg (EN AB-42000) Selection of Aluminum Alloys, Volume 2B, ASM Handbook, EN 1676:2020 ASM International, 2019, p 550. ISO 17615:2007 ISO AB-Al Si7Mg JIS H 2211:2010 AC4C.1, AC AlSi7Mg Supplier Castings Alloy 356.0 (UNS A03560) Raffmetal S.p.A. Via Malpaga, 82 ASTM B26/B26M:2018e1 EN AC-Al...
Journal Articles
Alloy Digest (1982) 31 (1): Al-235.
Published: 01 January 1982
... ALUMINUM 355.0 is a general-purpose, high-strength casting alloy containing silicon and copper as the major alloying elements. Its casting characteristics are excellent and it is recommended for pressure-tight castings. It can be age hardened and has good resistance to corrosion. Among its uses...
Journal Articles
Alloy Digest (1975) 24 (11): Al-219.
Published: 01 November 1975
... FEDERATED F150.5 is a heat-treatable aluminum alloy containing silicon and copper as the major alloying elements. It is recommended for high-strength, light-weight, pressure-tight castings. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile...