Alloy Digest (1974) 23 (8): Al-58.
Published: 01 August 1974
... ALUMINUM 2017 is an age-hardenable wrought alloy of medium strength and ductility. Its service temperature is below 212 F. It is used for general engineering applications, such as transportation equipment, machine parts and fittings. This datasheet provides information on composition, physical...
Journal Articles
Alloy Digest (1998) 47 (11): Al-355.
Published: 01 November 1998
... Kaiser Aluminum alloy 2017 has good machinability and good mechanical properties. It is used in rivets. General structural applications, and transportation. This datasheet provides information on composition, physical properties, hardness, tensile properties, and shear strength as well as fatigue...
Journal Articles
Alloy Digest (1979) 28 (11): Al-158.
Published: 01 November 1979
... of this alloy are widely used in aircraft and are also used successfully in other types of structures where the parts to be joined are Ahuninum 2014, Aluminum 2017 or Aluminum 2024. Forms Available: Rod, wire and rivets. Application: Rivets and other fasteners. Manufacturers: Aluminum alloy mills. ...
Journal Articles
Alloy Digest (2017) 66 (3): Ni-728.
Published: 01 March 2017
... that is precipitation hardened. It is used at high temperatures. Chemical Composition, wt (Nominal) Nickel 37.0 41.0 Chromium 17.0 19.0 Molybdenum 4.75 5.75 Titanium 2.2 2.5 Aluminum 0.7 1.0 Carbon 0.03 0.08 Cobalt 1.0 max Copper 0.5 max Manganese 0.2 max Silicon 0.5 max Sulfur 0.015 max Boron 0.001 max Zirconium 0.02...
Journal Articles
Alloy Digest (2017) 66 (1): Al-451.
Published: 01 January 2017
...-451. Producer or source: Kaiser Aluminum Corporation. Producer or Source: Kaiser Aluminum Corporation Copyright © ASM International® 2017 2017 ASM International chemical composition elasticity fatigue properties hardness hydraulic lines joinability KAISER ALLOY 5052 machinability...
Journal Articles
Alloy Digest (2017) 66 (2): Al-452.
Published: 01 February 2017
..., machining, and joining. Filing Code: Al-452. Producer or source: Kaiser Aluminum Corporation. Producer or Source: Kaiser Aluminum Corporation Copyright © ASM International® 2017 2017 ASM International chemical composition corrosion-resistant alloys elasticity fatigue properties hardness...
Journal Articles
Alloy Digest (2017) 66 (2): Cu-857.
Published: 01 February 2017
..., elasticity, tensile properties, and bend strength. It also includes information on forming and heat treating. Filing Code: Cu-857. Producer or source: Kobe Steel Ltd, Aluminum and Copper Business. Producer or Source: Kobe Steel Ltd, Aluminum and Copper Business Copyright © ASM International® 2017 2017...
Journal Articles
Alloy Digest (2017) 66 (5): Co-127.
Published: 01 May 2017
... available for trial evaluations. Applications: The typical application is in equipment used at high temperatures. Haynes NS-163 is a new developmental cobalt alloy for use up to 1204 °C (2200 °F). Chemical Composition, wt Chromium 28 Nickel 8 Iron 21 Manganese 0.5 max Niobium 1 Aluminum 0.5 max Titanium 1.3...
Journal Articles
Alloy Digest (2017) 66 (1): Cu-855.
Published: 01 January 2017
... properties, hardness, elasticity, tensile properties, and bend strength. It also includes information on forming and heat treating. Filing Code: Cu-855. Producer or source: Kobe Steel Ltd, Aluminum and Copper Business. Producer or Source: Kobe Steel Ltd, Aluminum and Copper Business Copyright © ASM...
Journal Articles
Alloy Digest (2017) 66 (3): Cu-858.
Published: 01 March 2017
... information on forming. Filing Code: Cu-858. Producer or source: Kobe Steel Ltd, Aluminum and Copper Business. Producer or Source: Kobe Steel Ltd, Aluminum and Copper Business Copyright © ASM International® 2017 2017 ASM International chemical composition elasticity hardness KOBELCO CAC...
Journal Articles
Alloy Digest (2017) 66 (3): Ni-727.
Published: 01 March 2017
... nickel alloys Haynes HR-224 is a new alloy with excellent oxidation resistance and improved fabricability and weldability compared to Haynes 214 alloy. Chemical Composition, wt (Maximum) Chromium 20 Molybdenum 0.5 Iron 27.5 Cobalt 2 Tungsten 0.5 Manganese 0.5 Silicon 0.3 Niobium 0.15 Aluminum 3.8...
Journal Articles
Alloy Digest (2017) 66 (1): TS-738.
Published: 01 January 2017
... Böhler (or Boehler) S630 tungsten-molybdenum HSS material similar with aluminum (similar to M2) has excellent toughness and cutting properties. This datasheet provides information on composition, physical properties, hardness, and elasticity. It also includes information on heat treating...
Journal Articles
Alloy Digest (2017) 66 (12): Cu-867.
Published: 01 December 2017
... (1769) Solidus temperature, °C (°F) 950 (1742) Magnetic permeability 1.003 Electrical Conductivity. International Annealed Copper Standard (IACS), depends on temper. Copyright © 2017, ASM International®. All rights reserved. KEMPER C688 (Zinc-Aluminum Copper Alloy) Filing Code: Cu-867 Copper :: December...
Journal Articles
Alloy Digest (2017) 66 (1): Al-450.
Published: 01 January 2017
... © 2017, ASM International®. All rights reserved. ALCOA 2099-T86 (Aluminum-Lithium Alloy) Filing Code: Al-450 Aluminum :: January 2017 Materials Park, Ohio 44073-0002 :: 440.338.5151 :: Fax 440.338.8542 :: www.asminternational.org :: [email protected] Published by ASM...
Journal Articles
Alloy Digest (2017) 66 (3): Al-455.
Published: 01 March 2017
... reserved. ALCOA 2624-T351 and 2624-T39 (Sheet/Plate Alloy) Filing Code: Al-455 Aluminum :: March 2017 Materials Park, Ohio 44073-0002 :: 440.338.5151 :: Fax 440.338.8542 :: www.asminternational.org :: [email protected] Published by ASM International® :: Data shown are typical...
Journal Articles
Alloy Digest (2017) 66 (2): Al-453.
Published: 01 February 2017
... Copyright © 2017, ASM International®. All rights reserved. ALCOA ALCLAD 2029 (Alclad Sheet/Plate Alloy) Filing Code: Al-453 Aluminum :: February 2017 Materials Park, Ohio 44073-0002 :: 440.338.5151 :: Fax 440.338.8542 :: www.asminternational.org :: [email protected] Published by ASM...
Journal Articles
Alloy Digest (2017) 66 (3): Al-454.
Published: 01 March 2017
...: Lamineries Matthey SA Copyright © ASM International® 2017 2017 ASM International chemical composition corrosion-resistant alloys elasticity hardness joinability machinability PERALUMAN 300 physical properties surface properties tensile properties workability wrought aluminum alloys...
Journal Articles
Alloy Digest (2017) 66 (11): TS-743.
Published: 01 November 2017
... (rotating bending fatigue test by Ono method) Fig. 2 Tensile strength at elevated temperature DOI: 10.31399/asm.ad.ts0743 Applications: General use in hot forging dies with hardness HRC 45 50. General use in extrusions dies with hardness HRC 45 49 in aluminum extrusion for the die, container type, outer...
Journal Articles
Alloy Digest (2017) 66 (6): SA-787.
Published: 01 June 2017
... Chromium 2.3 2.7 Molybdenum 0.25 Nickel Vanadium 0.2 Aluminum Iron bal Mechanical Properties: The mechanical properties in the tempered state are shown in Table 1 for a variety of size ranges from 16 mm to 250 mm (0.6 9.8 in The general properties are shown below on empirical basis to 4. Core hardness...
Journal Articles
Alloy Digest (2017) 66 (12): SA-807.
Published: 01 December 2017
... increases as well. This reduces the precipitation of nitrides and results in a lower increase in hardness. The nitriding temperature should be below the tempering temperature in order to keep the core hardness from decreasing. Effect of the Alloying Elements. Of the nitride forming elements aluminum...