Alloy Digest (1974) 23 (2): Al-44.
Published: 01 February 1974
... ALUMINUM 1100 is commercially pure aluminum and is characterized by its excellent ability to be drawn, spun, stamped or forged. It has good weldability, excellent resistance to corrosion and many home, architectural and industrial applications. This datasheet provides information on composition...
Journal Articles
Alloy Digest (1961) 10 (6): Al-104.
Published: 01 June 1961
... ALUMINUM EC is of higher purity than commercial ALUMINUM 1100 and is the electrical conductivity grade. This datasheet provides information on composition, physical properties, elasticity, tensile properties, and shear strength as well as creep and fatigue. It also includes information on low and...
Journal Articles
Alloy Digest (2002) 51 (2): Al-375.
Published: 01 February 2002
... AlcoTech Weld Metal 1100 is a 99% minimum or high-purity aluminum welding product that does not respond to heat treatment. It is used to weld the aluminum base alloys 1100, 1060, 1070, 1080 and 1350. This datasheet provides information on composition, physical properties, hardness, tensile...
Journal Articles
Alloy Digest (2019) 68 (11): Al-459.
Published: 01 November 2019
... Kaiser Alloy 1100 is in the commercially pure wrought family (1000 or 1xxx series) of aluminum alloys. It is typically used in applications requiring maximum ductility and relatively low strength. It has good corrosion resistance, workability, and weldability. This datasheet provides information...
Journal Articles
Alloy Digest (2007) 56 (9): SA-572.
Published: 01 September 2007
... max Iron bal (a) Intentional alloying elements. The steel is grain refined. (b) Total aluminum See Table 1 for carbon equivalent values. Mechanical Properties: See Tables 2 and 3. Heat Treatment: This alloy obtains mechanical properties by a quenching process. Weldox 1100 is not suited for...
Journal Articles
Alloy Digest (2012) 61 (6): SA-654.
Published: 01 June 2012
... SuperElso 1100 is a high yield strength quenched and tempered steel alloy. For welded and weight-saving structures. This datasheet provides information on composition and tensile properties as well as fracture toughness. It also includes information on forming, machining, and joining. Filing Code...
Journal Articles
Alloy Digest (2016) 65 (12): SA-773.
Published: 01 December 2016
... Strenx 1100 MC is a high-strength hot-rolled structural steel made for cold forming, with minimum yield strength of 1100 MPa (160 ksi) for stronger and lighter structures. This alloy meets or exceeds the requirements of S1100 MC in EN 10149-2. This datasheet provides information on composition...
Journal Articles
Alloy Digest (2012) 61 (9): SA-663.
Published: 01 September 2012
... Dillimax 1100 is a high-strength, quenched and tempered, fine-grained structural steel with minimum yield strength of 1100 MPa (160 ksi). Its mechanical properties are achieved by water quenching followed by tempering. This datasheet provides information on composition, physical properties, and...
Journal Articles
Alloy Digest (2014) 63 (4): CS-183.
Published: 01 April 2014
... Optim 1100 QC (1100 MPa minimum yield strength) is a quenched (Q), cold formable (C) steel that exceeds most other materials with the tightest bend radius. The Optim family of alloys offers high strength and good workshop properties. This datasheet provides information on composition, physical...
Journal Articles
Alloy Digest (1973) 22 (10): Al-15.
Published: 01 October 1973
... TENZALOY is an aluminum casting alloy developed for its high-strength and self-aging characteristics for castings that must have good dimensional stability and good corrosion resistance. Large and small intricate castings can be made without the danger of distortion associated with heat treatment...
Journal Articles
Alloy Digest (1968) 17 (3): Al-173.
Published: 01 March 1968
... grease stick provides sufficient lubrication and prevents gumming the wheel. Workability: Readily formed. In rhe annealed state the forming quality is similar to aluminum 1100-O and 3003-O alloys; in the heat treated and heat treated plus aged tempers it forms more nearly like aluminum 1100 in rhe hard...
Journal Articles
Alloy Digest (1969) 18 (4): Al-186.
Published: 01 April 1969
... or 5356 or 5556. Workability: Readily formed. In the annealed temper the forming quality is similar to Aluminum 1100 and 3003 alloys; in the solution treated and solution treated plus aged temper, it forms more nearly like Aluminum 1100 in the hard temper. However, its formability is better than 6061...
Journal Articles
Alloy Digest (1973) 22 (6): Al-39.
Published: 01 June 1973
...-gas shielded arc by both the tungsten and consumable electrode method is generatly recommended. Corrosion Resistence: Aluminum 5052 has high corrosion resistance to atmosphere and salt water. It is more resistant to salt water than 1100 from the standpoint of the retention of both its mechanical...
Journal Articles
Alloy Digest (1973) 22 (12): Al-31.
Published: 01 December 1973
... mixture of lard oil and kerosene is generally used. Weldability: ALUMINUM 3003 is readily weldable by the torch, inert arc and electric resistance methods. Aiuminum 1100 flier rod is usually used when extra metal is required. For consumable electrodes Aluminum 1100 is recommended. Use 4043 filler rod when...
Journal Articles
Alloy Digest (1952) 1 (3): Al-3.
Published: 01 November 1952
... Aluminum 61S is a wrought, heat-treatable alloy that combines the qualities of excellent resistance to corrosion, ease of fabrication and good mechanical properties. (See update, Aluminum 6061, Alloy Digest Al-205, January 1973.) This datasheet provides information on composition, physical...
Journal Articles
Alloy Digest (1954) 3 (10): Al-21.
Published: 01 October 1954
... ALUMINUM 356 is a heat treatable aluminum casting alloy recommended for high strength, pressure-tight castings, and intricate shapes. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive and shear strength as well as...
Journal Articles
Alloy Digest (1954) 3 (7): Al-18.
Published: 01 July 1954
... ALUMINUM 355 is a heat treatable aluminum alloy containing silicon and copper as the major alloying elements. It is recommended for light weight, high strength, pressure tight castings. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile...
Journal Articles
Alloy Digest (1958) 7 (7): Al-67.
Published: 01 July 1958
... ALUMINUM 6151, formerly A51S Alloy, is an aluminum forging alloy combining good forgeability, strength, and resistance to corrosion. It responds to an age-hardening heat treatment. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties...
Journal Articles
Alloy Digest (1995) 44 (8): Al-338.
Published: 01 August 1995
... ALUMINUM ALLOY 771.0 can be sand or permanent mold cast and naturally aged at room temperature. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes information on casting, heat treating, machining, joining, and surface...
Journal Articles
Alloy Digest (1957) 6 (4): Al-50.
Published: 01 April 1957
... ALUMINUM 380 and A380 are copper-silicon types of aluminum die casting alloys having excellent castability and improved machinability. This datasheet provides information on composition, physical properties, elasticity, tensile properties, and shear strength as well as fatigue. It also includes...