Journal Articles
Alloy Digest (1979) 28 (8): Al-134.
Published: 01 August 1979
... ALUMINUM 1060 is a commercially pure grade of aluminum (99.6% minimum aluminum) recommended for applications requiring one or more of the following characteristics: excellent formability, excellent resistance to corrosion and excellent weldability. It has relatively low strength. It is recommended...
Journal Articles
Alloy Digest (1997) 46 (10): Al-342.
Published: 01 October 1997
... Lanxide 91-X-1060-30P is a metal-matrix composite (MMC) consisting of an aluminum-silicon magnesium alloy matrix and 30 vol.% of silicon carbide. The MMC is designed to outperform its unreinforced counterpart. It is available as sand castings with a T6 heat treatment. This datasheet provides...
Journal Articles
Alloy Digest (2002) 51 (2): Al-375.
Published: 01 February 2002
... AlcoTech Weld Metal 1100 is a 99% minimum or high-purity aluminum welding product that does not respond to heat treatment. It is used to weld the aluminum base alloys 1100, 1060, 1070, 1080 and 1350. This datasheet provides information on composition, physical properties, hardness, tensile...
Journal Articles
Alloy Digest (2005) 54 (7): Al-395.
Published: 01 July 2005
... is used primarily for electrical conductors. This alloy, when ordered in the H111 temper, exhibits the highest electrical conductivity of all extruded aluminum conductor grades, meeting or exceeding 61.0% IACS. Alloy 1060 has a 99.6% minimum aluminum content, 1100 has a 99.0% minimum aluminum content...
Journal Articles
Alloy Digest (2022) 71 (4): CS-220.
Published: 01 April 2022
... steels can be embrittled by contact with liquid brass, aluminum bronze, copper, zinc, lead-tin solders, lithium, cadmium and indium. The degree Table 1 Physical properties Property Liquidus temperature Density Coefficient of linear thermal expansion Thermal conductivity Specific heat capacity Electrical...
Journal Articles
Alloy Digest (2002) 51 (2): Ti-126.
Published: 01 February 2002
... shear strength tensile properties TIMETAL 679 workability thermal properties Chemical Composition, wt Tin 10.50 11.50 Zirconium 4.00 6.00 Aluminum 2.00 2.50 Molybdenum 0.80 1.20 Silicon 0.10 0.50 Iron 0.20 max Oxygen 0.20 max Hydrogen 0.0125 max Titanium bal Physical Properties: Density, kg/m3...
Journal Articles
Alloy Digest (2016) 65 (12): SA-774.
Published: 01 December 2016
... 0.75 Phosphorus 0.020 max Sulfur 0.020 max Aluminum, total 0.015 0.080 Boron 0.001 0.010 Chromium 0.90 1.20 Molybdenum 0.90 1.10 Nickel 0.20 max Vanadium 0.60 0.80 Titanium 0.07 0.15 Arsenic 0.020 max Tin 0.020 max Copper 0.20 max Antimony report R* 0.1 max *R = P + 2.43As + 3.57Sn + 8.16Sb + 0.13Cu...
Journal Articles
Alloy Digest (2002) 51 (8): Al-380.
Published: 01 August 2002
... 4.5 6.0 Iron 0.8 max Copper 0.30 max Manganese 0.05 max Magnesium 0.05 max Zinc 0.15 max Titanium 0.20 max Beryllium 0.0008 max Others, each 0.05 max Others, total 0.15 max Aluminum bal Physical Properties: Density, kg/m3 (lb/in.3 ) 2685 (0.097) Conductivity, O temper, %IACS 42 Melting range, °C (°F...
Journal Articles
Alloy Digest (1994) 43 (2): TS-523.
Published: 01 February 1994
... wheels with plenty of coolant. Restrict peripheral speed c. Polishing: Thyssen P20 SUPER (P20 Modified) has excellent polishability. The recommended technique after grinding to 600 grit is to finally polish with diamond paste or aluminum oxide power impregnated cloths.75,6O,45.30,15,9,6,3...
Journal Articles
Alloy Digest (1990) 39 (7): Al-305.
Published: 01 July 1990
..., tensile properties, and shear strength as well as fatigue. It also includes information on low and high temperature performance, and corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Al-305. Producer or source: Various aluminum companies. Producer or Source...
Journal Articles
Alloy Digest (1995) 44 (1): Al-331.
Published: 01 January 1995
... on high temperature performance and wear resistance. Filing Code: AL-331. Producer or source: Duralcan USA. Producer or Source: Duralcan USA Copyright © ASM International® 1996 1996 ASM International cast aluminum alloys chemical composition DURALCAN F3D.xxS elasticity fatigue properties...
Journal Articles
Alloy Digest (1955) 4 (4): Al-25.
Published: 01 April 1955
... ALUMINUM 4032, formerly known as Aluminium 32S, is a forging alloy having comparatively low coefficient of expansion and good forgeability. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive and shear strength as well...
Journal Articles
Alloy Digest (2006) 55 (5): TS-631.
Published: 01 May 2006
... steel, copper, or aluminum as work material; with thicker work material; or with high-strength work materials. This alloy is, however, also very suitable for blanking and forming of ultrahigh-strength steel sheet as these materials place high demands on the tool steel regarding abrasive wear resistance...
Journal Articles
Alloy Digest (2000) 49 (9): TS-580.
Published: 01 September 2000
... thermal properties BÖHLER K340 ISODUR has a balanced composition for cold work forming operations like stamping and cutting. Chemical Composition, wt (Nominal) Carbon 1.10 Silicon 0.90 Manganese 0.40 Chromium 8.30 Molybdenum 2.10 Vanadium 0.50 Aluminum and niobium Special additions Iron bal Physical...
Journal Articles
Alloy Digest (1984) 33 (1): Al-249.
Published: 01 January 1984
... Titanium Iron Silicon Copper Manganese Others, each total Aluminum 5.0-6.5 0.50-0.65 0.40-o. 6 0.15-o. 25 0.50 max. 0.30 max. 0.25 max. 0.10 max. 0.05 max. 0.20 max. Remainder Physical Constants: Density, Ib/cu in. (At 68 F) 0.101 g/cu cm (At 20°C) 281 Melting temperature, o F ( C) (Solidus) 1060 (570...
Journal Articles
Alloy Digest (1979) 28 (2): Al-126.
Published: 01 February 1979
... ALUMINUM 5056 is a non-heat-treatable wrought aluminum-magnesium-manganese-chromium alloy possessing high strength and ductility along with good hot and cold workability. It is recommended for such applications as rivets and screen wire. It may be used with or without cladding. This datasheet...
Journal Articles
Alloy Digest (2016) 65 (8): Al-445.
Published: 01 August 2016
...) Conductivity, 0 temper, 106 S/m (%IACS) 17 (29) Melting range, approximate, °C (°F) 571 638 (1060 1180) Anodize color White Mechanical Properties: See Table 1. Copyright © 2016, ASM International®. All rights reserved. ALCOTEC WELD FILLER WIRE 5356 (Al-Mg-Mn-Cr-Ti Weld Wire) Filing Code: Al-445 Aluminum...
Journal Articles
Alloy Digest (2002) 51 (4): Al-376.
Published: 01 April 2002
... Wire Corporation. Producer or Source: AlcoTec Wire Corporation Copyright © ASM International® 2002 2002 ASM International ALCOTEC WELD WIRE 5356 chemical composition joinability physical properties shear strength tensile properties wires wrought aluminum alloys thermal properties...
Journal Articles
Alloy Digest (2002) 51 (7): Cu-685.
Published: 01 July 2002
... 0.5 0.8 Iron 0.2 max Manganese 0.1 max Lead 0.1 max Zinc 0.2 max Tin 0.2 max Aluminum 0.04 max Phosphorus 0.005 max Magnesium 0.05 max Total, others 0.1 0.3 Copper bal Physical Properties: Density, kg/m3 (lb/in.3 ) 8802 (0.318) Melting range, °C (°F) 1040 1060 (1904 1940) Coefficient of linear thermal...
Journal Articles
Alloy Digest (1970) 19 (8): Al-198.
Published: 01 August 1970
... KO-1 ALLOY is an aluminum alloy for general casting purposes. It is used where high strength at room or elevated temperatures and high energy absorption are important. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and shear...