Alloy Digest (1989) 38 (5): Cer-3.
Published: 01 May 1989
... AlSiMag 222 is a porous ceramic material. It has excellent electrical insulating properties at elevated temperatures. For high frequency applications as an insulator, impregnation with a moisture repellant substance is required. AlSiMag 222 is well suited to prototype model making. This datasheet...