Alloy Digest (1989) 38 (12): Ni-377.
Published: 01 December 1989
... ALLVAC I-700 is a nickel-base alloy solid-solution strengthened by appreciable additions of cobalt, chromium and molybdenum. It is precipitation hardenable by virtue of aluminum and titanium additions. It is produced by vacuum induction melting followed by vacuum are remelting. This datasheet...
Journal Articles
Alloy Digest (1990) 39 (2): Ni-379.
Published: 01 February 1990
... AND ALLOYS &Copyright 1990, Atby @est. Inc. Ail fights msd. Publishedby: Ailoy Digest. Ire /x)1-677-9161 Datashownarat@cat,nottobersedfa 2-t cilnfield Street Orsngs. N.J. 07050 I U.SA s$mc#ii (K timl design. ALLVAC 80A ALLVAC 80A is an 80% Ni/20% Cr alloy which is strengthened by precipitation hardening...