Skip Nav Destination
Close Modal
Search Results for
ALLOY VMS-513
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Subjects
Journal
Article Type
Date
Availability
1-1 of 1 Search Results for
ALLOY VMS-513
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
Sort by
Journal Articles
Alloy Digest (1975) 24 (1): Ni-213.
Published: 01 January 1975
... ALLOY VMS-513 is a nickel-base alloy developed to meet the tough operating conditions of gasoline and diesel engines. It combines high-temperature strength with good resistance to corrosion and wear, plus good fatigue strength. It is used in valves for gasoline-fueled industrial engines...
Abstract
View article
PDF
ALLOY VMS-513 is a nickel-base alloy developed to meet the tough operating conditions of gasoline and diesel engines. It combines high-temperature strength with good resistance to corrosion and wear, plus good fatigue strength. It is used in valves for gasoline-fueled industrial engines. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as creep. It also includes information on high temperature performance, corrosion and wear resistance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: Ni-213. Producer or source: Simonds Steel Division, Wallace-Murray Corporation.