Journal Articles
Alloy Digest (1984) 33 (12): SA-404.
Published: 01 December 1984
... Alloy Steel 3.5Ni-1.8Cr-0.4Mo-0.1V is highly suitable for massive components, usually more than four inches thick. It has high hardenability which in a water-spray or water-immersion quench contributes to the formation of sizeable amounts of martensite along with some bainite, and possibly...