1-20 of 156

Search Results for ALLOY S-590

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Alloy Digest (1956) 5 (1): SS-39.
Published: 01 January 1956
... ALLOY S-590 is designed for service in the range of 1100-1400 F for applications where high strength and corrosion resistance are required. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness, creep...
Journal Articles
Alloy Digest (2004) 53 (3): SA-532.
Published: 01 March 2004
..., and ability to resist fatigue has driven this substitution. Today s applications include front and rear rails, crush cans, rocker reinforcements, b/c pillar reinforcements, cowl inner/outer, back panels, cross members, bumpers, and door intrusion beams. DUAL-TEN is a trademark of U.S. Steel Corporation. Fig...
Journal Articles
Alloy Digest (2009) 58 (1): SA-590.
Published: 01 January 2009
... standards: SMAW GMAW FCAW SAW wire flux EN EN 499 EN 440 EN 758 EN 756/EN 760 E 42 X X X H5 G 42 X X T 42 X X H5 S 42 X X AWS A5.5 A5.18 A5.20 A5.17 E 70xx ER 70 S-x E 7xT5-x F7P4-Exxx See also Fig. 1. Fig. 1 Underbead hardness in HAZ Corrosion Resistance: CarElso 70 SOHIC is a reproducible and clean steel...
Journal Articles
Alloy Digest (1993) 42 (12): SS-557.
Published: 01 December 1993
...) (in/rev) Center Periphery 0.80 590-690 0.004 C6 C7 1.20 590-690 0.005 C6 C7 1.60 590-690 0.006 C6 C7 2.00 590-690 0.008 C6 C7 Notes: Curling Fluid-Pressure: 2-44 psi Amount: %.5 gal/min Cuuing dala for indexable insen drills are highly dependent on make of drill; Ihe manufacturer s recommendations should...
Journal Articles
Alloy Digest (2017) 66 (3): Cu-858.
Published: 01 March 2017
... ( circular-mil/ft) 0.05027 (30) Electrical conductivity, 20 °C (68 °F), 106 S/m (%IACS) Temper H/SP 20 (34) Temper EH/SP 23 (40) Mechanical Properties: Modulus of elasticity, GPa (106 psi) 130 (19) Poisson s ratio 0.33 Copyright © 2017, ASM International®. All rights reserved. KOBELCO CAC 5 (High Stress...
Journal Articles
Alloy Digest (2013) 62 (4): SA-675.
Published: 01 April 2013
... Classification of welding consumables SMAW GMAW FCAW Wire-flux combination SAW AWS SFA 5-11 SFA 5-14 SFA 5-14 E NiCrMo-3 (625) ER NiCrMo-3 (625) ER NiCrMo-3 (625) E NiCrMo-4 (276) E NiCrMo-4 (276) E NiCrMo-4 (276) E NiCrMo-6 EN ISO 14172 ISO 18274 ISO 14172 ISO 18274 E Ni 6625 (625) S Ni 6625 (625) E Ni 6625...
Journal Articles
Alloy Digest (2002) 51 (7): Cu-685.
Published: 01 July 2002
... 16 (9) expansion, 20 200 °C (68 392 °F), 10 6/K (10 6/°F) Specific heat capacity, 381 (0.091) J/kg K (Btu/lb °F) Thermal conductivity at 20 °C 23.8 (13.7) (68 °F), W/m K (Btu/(ft h °F)) Electrical conductivity Unspecified sample at 20 °C 14 (24) (68 °F), 106 S/m (%IACS) Resistivity, 20 °C...
Journal Articles
Alloy Digest (2001) 50 (9): TS-590.
Published: 01 September 2001
... Lanark is a silicon-manganese shock resistant tool steel with highest impact strength of the AISI S type tool steels. It is used for pneumatic tools, shear blades, and mandrels. This datasheet provides information on composition, physical properties, hardness, and elasticity. It also includes...
Journal Articles
Alloy Digest (1993) 42 (9): SS-549.
Published: 01 September 1993
... dependent on make of drill; the manufacturer s recommendations should be considered. DOI: 10.31399/asm.ad.ss0549 Copyright © ASM International® 1996 Table 3 -TURNING DATA FOR PRODEC 316 cutting speed (sfm) Curting Cemented carbides Feed depth High speed (in/m ) (id C7 C6 C5 sreel -0.012 -0.08 785 625 - 98...
Journal Articles
Alloy Digest (2015) 64 (1): SS-1198.
Published: 01 January 2015
... Properties: Hardness values, typical, average (5) HV10 210 260 HB 210 240 HRC 15 20 Young s modulus, E, GPa (106 psi) 20 °C (68°F) 200 (29) 20 100 ºC (68 212 ºF) 190 (28) 20 200 ºC (68 392 ºF) 180 (26) 20 300 ºC (68 572 ºF) 170 (25) Shear modulus, G, GPa (106 psi) 20 °C (68°F) 75 (10.9) 20 100 ºC (68 212 ºF...
Journal Articles
Alloy Digest (2020) 69 (2): CI-66.
Published: 01 February 2020
... in compression MPa (ksi) 520 (75.4) Limit of proportionality(a) MPa (ksi) 170 (24.6) Bending strength MPa (ksi) 590 (85.5) Torsional strength MPa (ksi) 460 (66.7) Modulus of elasticity(a) GPa (106 psi) 145 (21.03) Modulus of rigidity GPa (106 psi) 65 (9.4) Modulus of rupture MPa (ksi) 640 (92.8) Poisson s ratio...
Journal Articles
Alloy Digest (2005) 54 (5): SS-929.
Published: 01 May 2005
... °C (752 °F) 22 (12.7) 500 °C (932 °F) 23 (13.3) Resistivity, room temperature, µ m ( circular-mil/ft) 0.80 (481) Specific heat capacity, room temperature, J/kg K (Btu/lb °F) 460 (0.11) Magnetic Yes Mechanical Properties: Shear modulus, room temperature, GPa (106 psi) 77 (11) Young s modulus...
Journal Articles
Alloy Digest (2013) 62 (5): SS-1145.
Published: 01 May 2013
... expansion, , 10 6/K (10 6/°F) °C (°F) Thermal conductivity, W/m·K (Btu/ (h·ft·°F)) Young s modulus, E, GPa (106 psi) 0 100 (32 212) 10.8 (6.0) 20 (68) 14 (8.1) 197 (29) 0 200 (32 392) 11 (6.1) 100 (212) 16 (9.2) 193 (28) 0 300 (32 572) 11.3 (6.3) 200 (392) 18.5 (10.7) 186 (27) 0 400 (32 752) 11.6 (6.4) 300...
Journal Articles
Alloy Digest (2000) 49 (7): TS-578.
Published: 01 July 2000
.... Producer: Böhler 2340 S. Arlington Heights Rd, Unit 200 Arlington Heights, IL 6005 (847) 228-7370 or (860) 638-2520 (847) 228-6310 (fax) ISSN: 002-614X TS-578B Table 1 Recommendations for Machining, Annealed Condition Depth of cut Feed Cutting speed Tool Operation in. mm ipr mm/rev fpm m/min U.S. grade ISO...
Journal Articles
Alloy Digest (1960) 9 (10): TS-98.
Published: 01 October 1960
... cutting-cdgc angle, and a nose radius of about 10% of depth of cut. Sintered carbide cutting tools should be ground to 4-8 deg. side rake, O-10 deg. back rake, 6-10 deg. side relief, 6-12 deg. end relief, 8-13 deg. end cutting-edge angle, lo-20 deg. side cutting-edge angle, and s nose radius equal to l/32...
Journal Articles
Alloy Digest (1999) 48 (8): SS-758.
Published: 01 August 1999
... Steel August 1999 URANUS 45NMo Temperature Young s modulus Shear modulus °C °F GPa 106 psi GPa 106 psi 20 68 200 29 75 10.9 100 212 190 28 73 10.5 200 392 180 27 70 10.1 300 572 170 26 67 9.7 See also Table 2. Table 1 Thermal and Electrical Properties Resistivity Thermal conductivity Specific heat...
Journal Articles
Alloy Digest (1998) 47 (7): SS-725.
Published: 01 July 1998
..., and equipment for thermomechanical pulping. Producer: Avesta Sheffield, Inc. Schaumburg. IL 60173 (800) 833-8703 (800) 545-8617 (fax) In Sweden: Avesta Sheffield AB PO. Box 16377 Stockholm, Sweden S-10327 46086133600 4608208481 (fax) ISSN: 002-614X SS-725B ...
Journal Articles
Alloy Digest (2020) 69 (8): CI-72.
Published: 01 August 2020
..., push-pull 28(c) 4.06(c) (a) 25% of tensile strength. (b) 80% of 0.1% proof strength in compression. (c) 33% of fatigue limit Casting Characteristics Property Unit Value Minimum casting section thickness mm 20 (in.) (0.75) Patternmaker s contraction(a) % 1.0 1.4 Solid contraction mm/m (in./ft) 13 16...
Journal Articles
Alloy Digest (2002) 51 (9): Cu-688.
Published: 01 September 2002
... °F) Thermal conductivity at 159 (92) 20 °C (68 °F), W/m K (Btu/(ft h °F)) Electrical resistivity at 0.42 0.83 (253 499) 20 °C (68 °F), µ m ( circular-mil/ft) Electrical conductivity, 106 S/m 12 24 (20.8 41.5) (%IACS) Mechanical Properties: Modulus of elasticity, GPa (106 psi) 140 (20.3) See...
Journal Articles
Alloy Digest (1996) 45 (10): SS-658.
Published: 01 October 1996
... composition corrosion-resistant alloys elasticity hardness heat treatability joinability physical properties tensile properties workability thermal properties - DIGEST - DATA ON WORLD WIDE METALS A I Filing Code: S-658 4 Stainless Reel , m-L October 1996 ~~ - - MID ALLOYS 4 CARPENTER TYPE 409Cb...