Journal Articles
Publisher: Journals Gateway
Alloy Digest (1987) 36 (8): Fe-79.
Published: 01 August 1987
... NILO alloy 36 is a binary iron-nickel alloy having a very low and essentially constant coefficient of thermal expansion at atmospheric temperatures. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on high...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1975) 24 (12): Fe-55.
Published: 01 December 1975
... ALLOY 36 is an iron-36% nickel alloy with the lowest thermal coefficient of expansion among commercial alloys. It is recommended for applications that require very low dimensional changes with variations in temperature. Among many applications it is used for length standards, bimetals and tapes...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2021) 70 (9): Ni-775.
Published: 01 September 2021
... VDM 36 (Pernifer 36) is a binary iron-nickel alloy with a particularly low coefficient of linear thermal expansion. This alloy is used for applications where dimensional changes due to temperature variation must be minimized or in conjunction with high expansion alloys in applications where...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1979) 28 (8): Fe-58.
Published: 01 August 1979
... TECHALLOY 36 Alloy is an iron-nickel alloy that has a thermal expansion rate about 10% of the rate for carbon steel up to 400 F. It provides the lowest thermal expansion rate of all similar types of alloys. It has fairly good room-temperature mechanical properties in the annealed condition...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2004) 53 (8): Fe-131.
Published: 01 August 2004
... Carpenter Invar 36 alloy is a 36% nickel-iron alloy with a rate of thermal expansion approximately one-tenth that of carbon steel at temperatures up to 204 deg C (400 deg F). This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1959) 8 (3): Co-17.
Published: 01 March 1959
... HAYNES Alloy No. 36 is a cobalt-base alloy having excellent strength at temperatures up to 1800 deg. F. It is the cast modification of wrought HAYNES Alloy No. 25 and has been used successfully in jet engine blading and nozzle vanes. This datasheet provides information on composition, physical...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2012) 61 (2): Fe-158.
Published: 01 February 2012
... SSC Invar 36 was developed for use in applications where dimensional stability is essential. It is a nickel-iron alloy with a very low coefficient of thermal expansion from cryogenic temperatures to 200 deg C (390 deg F). It is utilized in aerospace composite tooling and die applications, as well...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2012) 61 (4): Fe-159.
Published: 01 April 2012
... Supra 36 is a Fe-Ni alloy with 36% nickel content that exhibits the highest electrical resistivity in the Fe-Ni system. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes information on forming, heat treating, and machining...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1958) 7 (6): Al-66.
Published: 01 June 1958
... APEX 36 is a high silicon, aluminum die casting alloy having high fluidity, excellent castability and good corrosion resistance. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and shear strength as well as fracture toughness...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1970) 19 (6): Fe-43.
Published: 01 June 1970
... UNISPAN 36 is a 36% nickel-iron alloy having low thermal expansion in a -400 F to +350 F range. It is recommended for parts in precision machinery and for applications where dimensional changes due to temperature variation must be minimized. This datasheet provides information on composition...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1964) 13 (5): Cb-8.
Published: 01 May 1964
... COLUMBIUM D-36 is a readily fabricable, moderate strength columbium-base alloy for high temperature service. This alloy is double consumable-electrode vacuum arc melted. It has a strength to density ratio at 2000 F (stress-relieved sheet) of 80500. This datasheet provides information...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2011) 60 (8): Fe-154.
Published: 01 August 2011
... NAS 36 is a nickel-iron alloy with a low coefficient of thermal expansion and is sensitive to changes in size. This datasheet provides information on composition, physical properties, and elasticity. It also includes information on corrosion resistance as well as forming. Filing Code: Fe-154...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1996) 45 (8): Fe-111.
Published: 01 August 1996
... Magnifier 36 is a soft-magnetic nickel-iron alloy with 36% nickel. It has a saturation induction of 1.3 T and a rather high electrical resistance of 0.75 0.75 ohm mm 2 /m. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1984) 33 (6): Bi-36.
Published: 01 June 1984
..., machining, and joining. Filing Code: Bi-36. Producer or source: Producers of low-melting alloys. Producer or Source: Producers of low-melting alloys Copyright ┬ę ASM International┬« 1996 1996 ASM International BISMUTH-22.6Pb-19.1In-8.3Sn-5.3Cd castability chemical composition eutectic systems...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2008) 57 (1): Fe-143.
Published: 01 January 2008
... Invar is an Fe-Ni alloy with 36% Ni content that exhibits the lowest expansion of known metals from very low temperatures up to approximately 230 deg C (445 deg F). Invar M93 is a cryogenic Invar with improved weldability. This datasheet provides information on composition, physical properties...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1981) 30 (6): Zn-36.
Published: 01 June 1981
... Tg 27 Zinc Alloy Filing Code: Zinc Alloy Zn-36 JUNE 1961 - DATA ON WORLD WIDE METALS AND ALLOYS @ Copyright 1980, Engineering Publication& Inc. Ail rights reserved. ISSN : 002-6 14X Publidml by Engineering Alloys Digest, inc. Post Office Box 823 Upper Montclair, New Jersey Tg 27 Zinc Alloy (Zinc-Base...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1990) 39 (4): Fe-90.
Published: 01 April 1990
... be cold formed due to its high silicon content. This alloy was covered with 4 other silicon core irons in Fe-36, November, 1968. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes information on heat treating and machining. Filing...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1957) 6 (8): Ni-36.
Published: 01 August 1957
... joinability low-temperature alloys machinability physical properties tensile properties workability Filing a Ni-36 HASTELLOY ALLOY B Nickel Alloy % AUGUST 1957 DIGEST -DATA ON WORLD WIDE METALS AND ALLOYS P#bEhd &7 Engineering AIloys Digcsc. Inc Upper Montclair, New Jersey HASTELLOY* ALLOY B...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1955) 4 (8): Fe-8.
Published: 01 August 1955
... NILVAR is a 36% nickel-iron alloy having the lowest coefficient of expansion, recommended for applications requiring no dimensional changes with temperature variations. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1996) 45 (6): Fe-110.
Published: 01 June 1996
... Magnifer 36K is a soft-magnetic nickel-iron alloy with 36% nickel. It has a saturation induction of 1.3 T and a rather high electrical resistance of 0.75 ohm mm 2 /m. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes...