Alloy Digest (1959) 8 (3): SA-81.
Published: 01 March 1959
... ALLOY 300M is an alloy steel offering a combination of hardenability, ductility and toughness at tensile strengths from 280,000 to 320,000 psi. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and bend strength as well as fracture...
Journal Articles
Alloy Digest (1993) 42 (2): SA-321.
Published: 01 February 1993
... LESCALLOY 300M VAC ARC is a low-alloy steel with an excellent combination of high hardenability and high strength coupled with good ductility and good toughness. Its tensile strength ranges from 280,000 to 300,000 psi. It is produced by the vacuum consumable electrode melting process to provide...
Journal Articles
Alloy Digest (2015) 64 (3): SA-722.
Published: 01 March 2015
... Lescalloy 300M-HS VAC-ARC is a clean high-strength, low-alloy steel with high strength, fracture toughness, and hardenability. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes information on forming, heat treating...
Journal Articles
Alloy Digest (2008) 57 (12): SS-942.
Published: 01 December 2008
... ultrahigh-strength steels such as 300M and SAE 4340 with corrosion resistance similar to 15-5 PH. The alloy is described as a nickel- and cobalt- containing secondary hardening stainless steels. The key structural features of Ferrium S53 alloy are a strong and tough fine lath martensite matrix, fine grain...
Journal Articles
Alloy Digest (2008) 57 (12): SA-589.
Published: 01 December 2008
...) aerospace grade. SAE committee F on corrosion and heat resistant alloys approved the specification for S53 premium aircraft-quality alloy steel. The specification itself covers material chemistry, processing, heat treatment, and minimum property requirements as shown below. 300M S53 Tensile strength, MPa...
Journal Articles
Alloy Digest (2008) 57 (12): SS-1003.
Published: 01 December 2008
... by normalizing and annealing. Machinability: This alloy is comparable in machining to 300M at a hardness of 35 HRC. Slightly reduced feeds and speeds may be necessary. Corrosion Resistance: The following four-level rating scale is intended by the producer for comparative purposes only. Corrosion testing...
Journal Articles
Alloy Digest (2018) 67 (9): SA-822.
Published: 01 September 2018
... and plate are also available upon request Applications M54 steel is being used in demanding applications in the aerospace, energy, oil and gas, and racing industries as an upgrade in performance from Maraging 250, 4340, 300M (BS S155), and other steels to reduce component weight or size or increase service...
Journal Articles
Alloy Digest (2014) 63 (5): SS-1171.
Published: 01 May 2014
... (120) 300M 302 (575) 65.9 (60) Pyrowear 675 316 (600) 164.8 (150) CBS600 316 (600) 98.9 (90) CSS42L 496 (925) 148.7 (135.3)(a) CBS-50 NiL 524 (975) 57.1 (52) M50 538 (1000) 19.7 (18) (a) Invalid P max /Pq > 1.10 Heat Treatment: Carburizing cycle: Preoxidize at 954 ºC (1749 ºF). Not required when...
Journal Articles
Alloy Digest (1984) 33 (3): SA-398.
Published: 01 March 1984
...% Offset) Crack Growth Rate Alloy* ksi MPa in. /hour mm/hour - - AlSl Type HI I 230 1586 1.0 25.4 AISI 4340 225 1551 1.0 25.4 300M 250 I724 0. I 254 H P%.45C 240 1655 0.1 f0 0.01 2.54 to 0.25 D6AC 215 1482 0.1 f0 0.001 254 to 0.025 250 Maraging 240 1655 0.01 to 0.001 0.25 to 0.025 300 Maraging 280 1931...