Alloy Digest (1955) 4 (6): SS-30.
Published: 01 June 1955
... ALLEGHENY METAL 25-20B is an austenitic chromium-nickel stainless steel with the highest oxidation resistance of any of the chromium-nickel steels. It has been developed from AISI 310 by raising the silicon content in order to improve the resistance to oxidation and the resistance to carburization...