Alloy Digest (2001) 50 (7): SS-825.
Published: 01 July 2001
... ALLEGHENY LUDLUM TYPE 201L chemical composition corrosion-resistant alloys corrosivity hardness heat treatability physical properties tensile properties thermal properties UNS S20103 ALLEGHENY LUDLUM TYPE 201L (High Manganese Austenitic Stainless Steel) Type 201L is a low-carbon version of type...
Journal Articles
Alloy Digest (2007) 56 (9): SS-997.
Published: 01 September 2007
... Allegheny Ludlum Type 201 stainless steel has many properties similar to Type 301 and provides excellent strength and formability. Together, Type 201 and Type 201L (see Alloy Digest SS-825, July 2001) account for the greatest tonnage of Cr-Ni-Mn 200 series stainless steels. A typical application...