Alloy Digest (1992) 41 (4): Fe-97.
Published: 01 April 1992
... Allegheny Ludlum No. 2 and No. 5 relay steels are iron/silicon alloys. They are soft magnetic alloys that combine high magnetic permeability, low residual magnetization and low coercive force with good mechanical properties and fabricability. This datasheet provides information on composition and...
Journal Articles
Alloy Digest (1979) 28 (1): SS-360.
Published: 01 January 1979
... ALLEGHENY LUDLUM E-BRITE 26-1 ALLOY is a low-carbon, low-nitrogen ferritic stainless steel made by a vacuum refining process. It provides: (1) Excellent resistance to pitting and crevice corrosion in chloride-containing environments, (2) Excellent resistance to chloride stress-corrosion cracking...
Journal Articles
Alloy Digest (1985) 34 (8): SS-462.
Published: 01 August 1985
... intergranular corrosion in the ASTM A262 Practice E 16(r,sulfuric acid - copper sulfate test. Specification Equivalents: ASTM: A 240. A 276, A 789 and 4 790. ASME: SA 240. SA 789 and SA 790. UNS No. S31803. General Characteristics: Allegheny Ludlum AL 2205 Alloy is a recently developed duplex stainless steel...
Journal Articles
Alloy Digest (1956) 5 (1): SS-39.
Published: 01 January 1956
... steel.5 ate satisfactory ingcnua. Workabilityz Thfs alloy is roUed and forged from temperatures of 2100. 2250 deg. F. with a Iiberai soaking time. It has no hot- short range, but since work-hrdcning occurs even at high temperatures, hot working becomes vay acult at lowet tempemmtes and frequent n&earing...
Journal Articles
Alloy Digest (1998) 47 (7): SS-723.
Published: 01 July 1998
... Allegheny Ludlum type 301 is the basic 18-8 chromium-nickel austenitic stainless steel with both chromium and nickel content lower than types 302 and 304. The steel is capable of attaining high tensile strength with good ductility by moderate or severe cold working. A typical application is...
Journal Articles
Alloy Digest (1979) 28 (3): SS-362.
Published: 01 March 1979
... ALLEGHENY LUDLUM Type 29-4 is a low-interstitial ferritic stainless steel. It contains approximately 29% chromium and 4% molybdenum. The alloy provides excellent resistance to pitting, crevice corrosion, and stress-corrosion cracking in chloride-containing environments. Type 29-4 is used widely...
Journal Articles
Alloy Digest (1988) 37 (5): SS-494.
Published: 01 May 1988
... Allegheny Ludlum AL-6XN alloy is characterized as a superaustenitic stainless steel having an exceptional level of corrosion resistance, especially to chloride pitting. It has high strength and its impact value at room temperature is 140 ft-lb and at 320 F (196 C) is 85 ft-lb. It is covered by...
Journal Articles
Alloy Digest (1978) 27 (4): SS-349.
Published: 01 April 1978
... comparable data for ALdX and AISI Type 316. Weldability: Allegheny Ludlum AL-6X can be welded readily by the inert gas processes. Resistance to Corrosion and Oxidation: Allegheny Ludlum AL-6X is resistant to atmospheric corrosion and similar mild types of corrosion. In general, those media which have no...
Journal Articles
Alloy Digest (2002) 51 (1): SS-840.
Published: 01 January 2002
... seacoast exposure Base metal No cracking Welded No cracking Producer: Allegheny Ludlum Corporation Pittsburgh, PA 16222-6479 (800) 258-3586 (412) 252-3162 (fax) Technical inquiries (724) 226-6300 ISSN: 002-614X SS-840B ...
Journal Articles
Alloy Digest (1964) 13 (10): TS-153.
Published: 01 October 1964
... Allegheny Ludlum 602 is a manganese, silico-molybdenum type, shock resisting tool steel recommended for applications where extreme toughness is required along with hardness and wear resistance. This datasheet provides information on composition, physical properties, hardness, elasticity, and...
Journal Articles
Alloy Digest (1986) 35 (6): SS-470.
Published: 01 June 1986
... and Figure I). Being titanium stabilized, ALLEGHENY LUDLUM TYPE 439 resists intergranular attack (See Table 5). The alloy is also immune to ammoniacal stress corrosion or dissolution in boiler feedwater or steam. a condition that has led to early failure in some copper-base alloys. Type 439 is...
Journal Articles
Alloy Digest (2005) 54 (6): SS-923.
Published: 01 June 2005
... embrittlement processes observed above 540 °C (1000 °F) are diffusion controlled, and the minor compositional differences between AL-6XN PLUS alloy and the AL-6XN alloy have no influence on embrittlement susceptibility. ALLEGHENY LUDLUM AL-6XN PLUS Filing Code: SS-923 Stainless Steel Original April 2005...
Journal Articles
Alloy Digest (1971) 20 (6): TS-234.
Published: 01 June 1971
... ALLEGHENY LUDLUM EXOHARD is an ultrahard high-speed tool steel (AISI Type M47) suited for machining hard and otherwise difficult-to-machine materials. This datasheet provides information on composition, physical properties, and hardness as well as fracture toughness. It also includes information...
Journal Articles
Alloy Digest (1996) 45 (2): SS-639.
Published: 01 February 1996
... temperature performance and corrosion resistance as well as heat treating and joining. Filing Code: SS-639. Producer or source: Allegheny Ludlum Corporation. Producer or Source: Allegheny Ludlum Corporation Copyright © ASM International® 1996 1996 ASM International m(yy f!!J ==f~;a;~ - DIGEST - DATA...
Journal Articles
Alloy Digest (1996) 45 (5): SS-644.
Published: 01 May 1996
..., and tensile properties. It also includes information on high temperature performance and corrosion resistance as well as heat treating. Filing Code: SS-644. Producer or source: Allegheny Ludlum Corporation. Producer or Source: Allegheny Ludlum Corporation Copyright © ASM International® 1996...
Journal Articles
Alloy Digest (1997) 46 (10): SS-640.
Published: 01 October 1997
..., machining, and joining. Filing Code: SS-640. Producer or source: Allegheny Ludlum Corporation. Originally published March 1996, revised October 1997. Producer or Source: Allegheny Ludlum Corporation Copyright © ASM International® 1997 1997 ASM International Allegheny Ludlum Type 205 chemical...
Journal Articles
Alloy Digest (1986) 35 (12): SS-480.
Published: 01 December 1986
... ALLEGHENY LUDLUM AL 29-4-2 alloy is a high-purity ferritic stainless steel designated to provide superior resistance to corrosion by aggressive environments. It also offers fabrication characteristics that (along with E-BRITE Alloy) are unique among highly alloyed ferritic materials. The...
Journal Articles
Alloy Digest (1967) 16 (7): SS-196.
Published: 01 July 1967
... Allegheny Ludlum 419 is a ferritic (martensitic) type chromium-tungsten alloy recommended for high temperature applications in the temperature range of 800-1200 F, such as turbine and jet engine components. This datasheet provides information on composition, physical properties, elasticity...
Journal Articles
Alloy Digest (2007) 56 (11): SS-1001.
Published: 01 November 2007
...- phere involved, heating and cooling cycles, and structural design, no actual data can be presented that would apply to all conditions. Weight Change. See Table 2. Specification Equivalents: UNS S43000 ASTM A 240 General Characteristics: Allegheny Ludlum Stainless Type 430 is a low-carbon ferritic stain...
Journal Articles
Alloy Digest (1962) 11 (4): SS-130.
Published: 01 April 1962
... 1200 19000 12000 Rockwell Hardness C 45.0 38.0 32.0 27.5 27.0 DOI: 10.31399/asm.ad.ss0130 Copyright © ASM International® 1996 Hardening Temperature oF Table 5 - STANDARD IZOD IMPACT TESTS Tempering No. Irod Temperature of Impact Quench oF Quench Hours ft-lb - - - Rockwell Hardness C As annealed...