1-20 of 51 Search Results for

ALLEGHENY LUDLUM AL 800

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Alloy Digest (1998) 47 (4): SS-712.
Published: 01 April 1998
... corrosion resistance as well as forming, heat treating, and joining. Filing Code: SS-712. Producer or source: Allegheny Ludlum Corporation. Producer or Source: Allegheny Ludlum Corporation Copyright © ASM International® 1998 1998 ASM International ALLEGHENY LUDLUM AL 800 chemical composition...
Journal Articles
Alloy Digest (1998) 47 (5): SS-717.
Published: 01 May 1998
... 1998 ALLEGHENY LUDLUM AL 800HfM, AL (High-Temperature Austenitic Stainless Steel) AL 800H and AL 800AT are nickel-iron-chromium alloys designed to resist oxidation and carbutization at elevated temperatures. AL 800. AL 8OOH. and AL 800AT are trademarks of Allegheny Ludlum Corporation. Chemical...
Journal Articles
Alloy Digest (2005) 54 (6): SS-923.
Published: 01 June 2005
... (800) 289-7528 www.alleghenyludlum.com/ludlum/ ISSN: 002-614X SS-923B Table 3 Corrosion Performance CCCT CPT ECPT AL-6XN AL-6XN PLUS AL-6XN AL-6XN PLUS AL-6XN AL-6XN PLUS Test method Test solution Test surface °C °F °C °F °C °F °C °F °C °F °C °F ASTM G 48 Acidified ferric Pickled mill 43 109 55 131...
Journal Articles
Alloy Digest (1989) 38 (1): Ni-366.
Published: 01 January 1989
... Allegheny Ludlum AL 825 alloy is a nickel-iron-chromium-molybdenum-copper alloy with superior corrosion resistance including stress-corrosion cracking resistance. It is highly ductile from cryogenic to well over 1000 F(538 C) temperatures. It is readily weldable. This datasheet provides...
Journal Articles
Alloy Digest (2000) 49 (4): SS-780.
Published: 01 April 2000
... where type 304 is used. Producer: Allegheny Ludlum Corporation Pittsburgh, PA 15222-5479 (800) 258-3586 (412) 394-2805 (fax) ISSN: 002-614X SS-780B Table 2 Formability Values versus Thickness Strip n1/n2 R LDR thickness, in. AL 304DA Type 304 AL 304DA Type 304 AL 304DA Type 304 0.030 0.20/0.27 0.33/0.49...
Journal Articles
Alloy Digest (2000) 49 (12): SS-811.
Published: 01 December 2000
... on high temperature performance and corrosion resistance as well as joining. Filing Code: SS-811. Producer or source: Allegheny Ludlum Corporation. Producer or Source: Allegheny Ludlum Corporation Copyright © ASM International® 2000 2000 ASM International ALLEGHENY LUDLUM AL 611...
Journal Articles
Alloy Digest (2001) 50 (1): Fe-4.
Published: 01 January 2001
.... Producer or source: Allegheny Ludlum Corporation. Originally published as Allegheny 4750, February 1954, revised January 2001. Producer or Source: Allegheny Ludlum Corporation Copyright © ASM International® 2001 2001 ASM International Allegheny Ludlum AL 4750 chemical composition corrosion...
Journal Articles
Alloy Digest (2001) 50 (2): SS-819.
Published: 01 February 2001
... acid. Producer: Allegheny Ludlum Corporation Pittsburgh, PA 16222-6479 (800) 258-3586 (412) 252-3162 (fax) Technical assistance (724) 226-6300 ISSN: 002-614X SS-819B Table 4 Corrosion Data for AL 610 Sheet Corrosion rate, average Solution mm/yr mils/yr ASTM A 262 Practice B, ferric sulfate-sulfuric...
Journal Articles
Alloy Digest (2000) 49 (3): Ni-559.
Published: 01 March 2000
... Allegheny Ludlum AL 22 chemical composition corrosion-resistant alloys hardness joinability physical properties tensile properties wrought nickel alloys thermal properties UNS N06022 ALLEGHENY LUDLUM AL 22 (Nickel-Base Alloy) AL-22 is a wrought 22Cr-13.5Mo-3W-4Fe high-nickel alloy with...
Journal Articles
Alloy Digest (1989) 38 (9): Ni-374.
Published: 01 September 1989
... Allegheny Ludlum AL 400 is a ductile nickel-copper alloy with resistance to a variety of corrosive conditions. The alloy is not hardenable by heat treatment. It can be appreciably strengthened by cold work. This datasheet provides information on composition, physical properties, elasticity, and...
Journal Articles
Alloy Digest (1990) 39 (1): SS-511.
Published: 01 January 1990
... ALLEGHENY LUDLUM AL 904L Alloy is an austenitic stainless steel designed for middle to high level corrosion resistance. It is produced to low carbon levels for use in the welded condition. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile...
Journal Articles
Alloy Digest (1988) 37 (5): SS-494.
Published: 01 May 1988
... Allegheny Ludlum AL-6XN alloy is characterized as a superaustenitic stainless steel having an exceptional level of corrosion resistance, especially to chloride pitting. It has high strength and its impact value at room temperature is 140 ft-lb and at 320 F (196 C) is 85 ft-lb. It is covered by...
Journal Articles
Alloy Digest (1978) 27 (4): SS-349.
Published: 01 April 1978
... ALLEGHENY LUDLUM AL-6X is an austenitic chromium-nickel-molybdenum stainless steel specifically designed for outstanding resistance to pitting and crevice attack in chloride-containing solutions. It possesses good ductility, high impact values and good weldability. It is an ideal material for...
Journal Articles
Alloy Digest (1967) 16 (7): SS-196.
Published: 01 July 1967
... Allegheny Ludlum 419 is a ferritic (martensitic) type chromium-tungsten alloy recommended for high temperature applications in the temperature range of 800-1200 F, such as turbine and jet engine components. This datasheet provides information on composition, physical properties, elasticity...
Journal Articles
Alloy Digest (1996) 45 (4): SS-641.
Published: 01 April 1996
... AND ALLOYS @%pydghr 1996, ASM Imemationel. All rights reservedD63ataShOWl7~rypical.flOttOb used for epecaetion or fine/ design. Pub&bed bv: A.94 Imemetbnel Materids Park. Ohio 040734X02 21M38-5151 Fa.7216-2394634 h4em-Se~%po.AShWnL.0q ALLEGHENY LUDLUM OHMALOY@ 40 (Resistance Alloy) AL Ohmaloy 40 alloy...
Journal Articles
Alloy Digest (2007) 56 (10): SS-1000.
Published: 01 October 2007
... Allegheny Ludlum Type 201LN (AL 201LN) is a modification of Type 201 developed especially for cryogenic service to -195 deg C (-320 deg F) to handle industrial gases. Its strength and corrosion resistance also allow other applications. This datasheet provides information on composition, physical...
Journal Articles
Alloy Digest (1956) 5 (5): TS-46.
Published: 01 May 1956
... toughness. It also includes information on forming, heat treating, and machining. Filing Code: TS-46. Producer or source: Allegheny Ludlum Corporation. Producer or Source: Allegheny Ludlum Corporation Copyright © ASM International® 1996 1996 ASM International Allegheny AL 609 chemical...
Journal Articles
Alloy Digest (1996) 45 (2): SS-638.
Published: 01 February 1996
..., A479. A666 AMS 5562.5595.5656 General Characteristics: Allegheny Ludlum s AL 219 alloy, also known by the more familiar 21-6-9* designation and XM-11. is a nitrogen-bearing austenitic stainless steel that has substantially higher strength than standard austenitic stainless steels. The stable austenite...
Journal Articles
Alloy Digest (1996) 45 (1): Ni-497.
Published: 01 January 1996
... lntematicml Materials Park. Ohio 440734002 2163385151 Fax216-3384634 Mem-ServQpoASM-ln*org ALLEGHENY LUDLUM AL 276 (Ni-Mo-&Fe-W Corrosion Resistant Alloy) Allegheny Ludlum AL276 is widely used in the most severe environments found in chemical piants and in power plant desulfurization systems. The high...
Journal Articles
Alloy Digest (2000) 49 (2): SS-776.
Published: 01 February 2000
...: Allegheny Ludlum Corporation Pittsburgh, PA 15222-5479 (800) 258-3586 (724) 226-6300 (technical assistance) ISSN: 002-614X SS-776B ...