Publisher: Journals Gateway
Alloy Digest (2000) 49 (12): SS-811.
Published: 01 December 2000
... on high temperature performance and corrosion resistance as well as joining. Filing Code: SS-811. Producer or source: Allegheny Ludlum Corporation. Producer or Source: Allegheny Ludlum Corporation Copyright ┬ę ASM International┬« 2000 2000 ASM International ALLEGHENY LUDLUM AL 611 chemical...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2001) 50 (2): SS-819.
Published: 01 February 2001
... Allegheny Ludlum alloy AL 610 is an austenitic stainless steel alloy with a special composition including high silicon to specifically resist high concentrations of nitric acid. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also...