Alloy Digest (2001) 50 (2): SS-819.
Published: 01 February 2001
... Allegheny Ludlum alloy AL 610 is an austenitic stainless steel alloy with a special composition including high silicon to specifically resist high concentrations of nitric acid. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also...
Journal Articles
Alloy Digest (2000) 49 (12): SS-811.
Published: 01 December 2000
... on high temperature performance and corrosion resistance as well as joining. Filing Code: SS-811. Producer or source: Allegheny Ludlum Corporation. Producer or Source: Allegheny Ludlum Corporation Copyright ┬ę ASM International┬« 2000 2000 ASM International ALLEGHENY LUDLUM AL 611 chemical...
Journal Articles
Alloy Digest (1989) 38 (1): Ni-366.
Published: 01 January 1989
... Allegheny Ludlum AL 825 alloy is a nickel-iron-chromium-molybdenum-copper alloy with superior corrosion resistance including stress-corrosion cracking resistance. It is highly ductile from cryogenic to well over 1000 F(538 C) temperatures. It is readily weldable. This datasheet provides...
Journal Articles
Alloy Digest (1996) 45 (2): SS-638.
Published: 01 February 1996
.... A666 AMS 5562.5595.5656 General Characteristics: Allegheny Ludlum s AL 219 alloy, also known by the more familiar 21-6-9* designation and XM-11. is a nitrogen-bearing austenitic stainless steel that has substantially higher strength than standard austenitic stainless steels. The stable austenite...