Skip Nav Destination
Close Modal
Search Results for
ALLEGHENY LUDLUM AL 2205 ALLOY
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Subjects
Journal
Article Type
Date
Availability
1-2 of 2 Search Results for
ALLEGHENY LUDLUM AL 2205 ALLOY
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
Sort by
Journal Articles
Alloy Digest (1985) 34 (8): SS-462.
Published: 01 August 1985
... ALLEGHENY LUDLUM AL 2205 ALLOY is in the family of duplex alloys in which added nitrogen significantly improves corrosion resistance, especially in the welded condition. The microstructure consists of a balanced mixture of austenitic and ferritic phases. Its corrosion resistance to many...
Abstract
View article
PDF
ALLEGHENY LUDLUM AL 2205 ALLOY is in the family of duplex alloys in which added nitrogen significantly improves corrosion resistance, especially in the welded condition. The microstructure consists of a balanced mixture of austenitic and ferritic phases. Its corrosion resistance to many environments is superior to Types 316 or 317 and it has a yield strength more than double that of AISI conventional austenitic stainless steels. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness. It also includes information on corrosion resistance as well as forming, heat treating, and machining. Filing Code: SS-462. Producer or source: Allegheny Ludlum Corporation.
Journal Articles
Alloy Digest (2002) 51 (12): SS-869.
Published: 01 December 2002
...: SS-869. Producer or source: Allegheny Ludlum Corporation. Producer or Source: Allegheny Ludlum Corporation Copyright © ASM International® 2002 2002 ASM International AL 2003 chemical composition corrosion-resistant alloys elasticity fracture toughness hardness heat treatability...
Abstract
View article
PDF
The AL 2003 alloy is a nitrogen-enhanced leaner nickel and molybdenum alloy than the duplex stainless steel AL 2205, but is similar in both phase balance and mechanical properties. Applications include areas where resistance to both general and chloride-ion stress-corrosion cracking is important. This datasheet provides information on composition, physical properties, microstructure, hardness, elasticity, and tensile properties as well as fracture toughness. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, and joining. Filing Code: SS-869. Producer or source: Allegheny Ludlum Corporation.