1-8 of 8 Search Results for

ALLEGHENY A-286

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Alloy Digest (1966) 15 (9): SS-4.
Published: 01 September 1966
... ALLEGHENY A-286 is an austenitic iron-nickel-chromium alloy designed for service up to 1300 F where high strength and corrosion resistance are required, and for service at higher temperatures where the applications are for lower stresses. It is an age-hardenable alloy. This datasheet provides...
Journal Articles
Alloy Digest (2004) 53 (10): SS-911.
Published: 01 October 2004
... Allvac A-286 is an age-hardening austenitic stainless steel and a superalloy. Its high strength and corrosion resistance give it many applications including bolting. This datasheet provides information on composition, physical properties, hardness, and tensile properties as well as creep. It also...
Journal Articles
Alloy Digest (1998) 47 (4): SS-712.
Published: 01 April 1998
... stainless steels such as types 301,3CM,309, and 310. but not as strong as superal.loys such as Altemp A-286, Altemp l-IX. AL 625. or Altemp 718. See Alloy Digest SS-4. Ni-442, Ni-443. and Ni-444, respectively. Cold Formabiity. The AL 800 alloy exhibits excellent cold forming characteristics normally...
Journal Articles
Alloy Digest (1972) 21 (11): SS-282.
Published: 01 November 1972
... lOOOoF, temper 10500F temper 12OOoF, 3 hr, ac; temper minimum 2 hr, ac 960-lOOOoF, 3 hr, ac 160000 min. 134000- 160000 155000 min. 110000 min. 110000 min. 130000 min. 13 min. 17 min. 12 min. 30 min. - 30 min. - 45 min. 30 min. 40 min. - - 338-363 286-33 1 341-388 0.28 6.0 x lo-6 6.6 x 10-6 30-32 x A...
Journal Articles
Alloy Digest (1960) 9 (10): Ni-61.
Published: 01 October 1960
... deformation, a rapid work-hardening race at room temperature, low hardness in the solution treated or annealed condition, and high hardness after aging. The oxidation resistance of D-777 has been evaluated up CO 18000F in still air furnaces and found to be similar to Alloy A-286 at 12OOOF but superior to char...
Journal Articles
Alloy Digest (1954) 3 (7): TS-22.
Published: 01 July 1954
... ATLAS 93 is a chromium molybdenum shock resisting steel, having rather deep oil hardening characteristics with fairly high impact value. This datasheet provides information on composition, hardness, and tensile properties as well as fracture toughness. It also includes information on forming, heat...
Journal Articles
Alloy Digest (1993) 42 (10): Ni-442.
Published: 01 October 1993
...-solution strengthened. Applications include uses in the aerospace, heat treatment and petrochemical markets. @Ahemp is a registered trademark of Allegheny Ludlum Corp. Chemical Compositionl, Wt, %: Carbon Manganese Phosphorus Sulfur Silicon Chromium Molybdenum cobalt Tungsten Iron Nickel Typical 0.08 0.50...
Journal Articles
Alloy Digest (2002) 51 (12): Ni-595.
Published: 01 December 2002
... Nickelvac K-500 is a nickel-copper alloy with age-hardening properties imparted by alloying additions of aluminum and titanium. The alloy is characterized by excellent corrosion resistance in an extensive range of natural and chemical environments, excellent resistance to chloride-ion stress...