... AlgoTuf 440F is designed for wear resistance and is one in a full range of heat-treated plate products by Algoma Steel for construction, mining, manufacturing, and military applications. This datasheet provides information on composition, hardness, and tensile properties as well as fracture...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2004) 53 (1): CS-139.
Published: 01 January 2004
... Algoma 100/130 AlgoTuf 400F AlgoTuf 440F AlgoTuf 500 Cutting speed 390 in./min Cutting speed 360 in./min Cutting speed 360 in./min Cutting speed 1560 in./min Drill bit diameter, in. feed, in./rev rpm feed, in./rev rpm feed, in./rev rpm feed, in./rev rpm 1/4 0.019 497 0.014 458 0.011 458 0.004 1986 3/8...