Alloy Digest (2004) 53 (4): CS-142.
Published: 01 April 2004
... Algoma 100 is a cost-effective choice for applications that require high strength, improved notch toughness, weldability, and good formability. It is one in a full range of heat treated plate products for construction, mining, manufacturing, and military applications. This datasheet provides...
Journal Articles
Alloy Digest (2004) 53 (5): CS-143.
Published: 01 May 2004
... result. Weldability: Algoma 130 exhibits excellent weldability because of its low alloy content. This grade can be welded using simple procedures and common, readily available consumables. Algoma recom- mends low-hydrogen electrodes with a maximum of 10 mL per 100 g of weld deposit. High heat input...
Journal Articles
Alloy Digest (2004) 53 (1): CS-139.
Published: 01 January 2004
... Algoma 100/130 AlgoTuf 400F AlgoTuf 440F AlgoTuf 500 Cutting speed 390 in./min Cutting speed 360 in./min Cutting speed 360 in./min Cutting speed 1560 in./min Drill bit diameter, in. feed, in./rev rpm feed, in./rev rpm feed, in./rev rpm feed, in./rev rpm 1/4 0.019 497 0.014 458 0.011 458 0.004 1986 3/8...
Journal Articles
Alloy Digest (2004) 53 (2): CS-140.
Published: 01 February 2004
... AlgoTuf 440F is designed for wear resistance and is one in a full range of heat-treated plate products by Algoma Steel for construction, mining, manufacturing, and military applications. This datasheet provides information on composition, hardness, and tensile properties as well as fracture...
Journal Articles
Alloy Digest (2004) 53 (3): CS-141.
Published: 01 March 2004
... toughness. It also includes information on forming, heat treating, machining, and joining. Filing Code: CS-141. Producer or source: Algoma Steel Inc. Producer or Source: Algoma Steel Inc. Copyright © ASM International® 2004 2004 ASM International ALGOTUF 500F chemical composition fracture...
Journal Articles
Alloy Digest (2003) 52 (12): CS-138.
Published: 01 December 2003
... Algoma AR225 is a carbon steel developed primarily to supply a low-cost material for high-abrasion applications. It is furnished in the form of as-rolled plate with a relatively high carbon content (0.35-0.45%). AR-225 is sold on the basis of chemical analysis only; the number 225 signifies...
Journal Articles
Alloy Digest (2013) 62 (12): CS-176.
Published: 01 December 2013
.... This datasheet provides information on composition, hardness, and tensile properties as well as fracture toughness. It also includes information on forming, machining, and joining. Filing Code: CS-176. Producer or source: Essar Steel, Algoma Steel Inc.. Producer or Source: Essar Steel, Algoma Steel Inc...
Journal Articles
Alloy Digest (1964) 13 (1): SA-159.
Published: 01 January 1964
.... Filing Code: SA-159. Producer or source: Algoma Steel Corporation Ltd. Producer or Source: Algoma Steel Corporation Ltd Copyright © ASM International® 1996 1996 ASM International Algo-Loy 1317 chemical composition elasticity hardness heat treatability joinability machinability...