Alloy Digest (1992) 41 (3): SS-525.
Published: 01 March 1992
... ALFA I and ALFA II ALLOYS are 13% chromium ferritic stainless steels with 3 and 4% aluminum, respectively. These steels have superior oxidation resistance. Being ferritic they are not hardenable by heat treatment. This datasheet provides information on composition, physical properties, hardness...
Journal Articles
Alloy Digest (2003) 52 (12): SS-897.
Published: 01 December 2003
... Class I DIN 17470 Allegheny Ludlum ALFA-IV Product Forms Available: Strip (foil) in coil form Applications: Substrate for industrial or automotive catalytic converters and other high-temperature applications, such as furnace parts and electric heating elements Producer: Engineered Materials Solutions...
Journal Articles
Alloy Digest (2003) 52 (11): SS-892.
Published: 01 November 2003
.... Specification Equivalents: ASTM B 603 Class I DIN 17470 Allegheny Ludlum ALFA-IV Product Forms Available: Strip (foil) in coil form Applications: Applications include substrate for industrial or automotive cat- alytic converters and other high-temperature applications, such as furnace parts and electric heating...