Alloy Digest (1992) 41 (9): Al-326.
Published: 01 September 1992
... and physical properties. It also includes information on joining. Filing Code: Al-326. Producer or source: AlcoTec Wire Corporation. Producer or Source: AlcoTec Wire Corporation Copyright © ASM International® 1996 1996 ASM International ALCOTEC ALLOY R-A357.0 brazing filler metal wire chemical...