1-1 of 1 Search Results for

ALCOA ALLOY 2519-T87

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Alloy Digest (2000) 49 (6): Al-370.
Published: 01 June 2000
... information on joining. Filing Code: AL-370. Producer or source: Alcoa Mill Products Inc. Producer or Source: Alcoa Mill Products Inc. Copyright Ā© ASM InternationalĀ® 2000 2000 ASM International ALCOA ALLOY 2519-T87 chemical composition compressive strength joinability military vehicles...