Alloy Digest (2006) 55 (7): Al-399.
Published: 01 July 2006
... Mill Products Copyright ┬ę ASM International┬« 2006 2006 ASM International ALCOA 2124 PLATE chemical composition corrosion-resistant alloys creep properties fatigue properties fracture toughness heat treatability high-temperature alloys joinability machinability physical properties...
Journal Articles
Alloy Digest (2000) 49 (9): Al-372.
Published: 01 September 2000
... Alcoa 2024 was introduced by Alcoa in 1931 as the first alloy to have a yield strength approaching 345 MPa (50 ksi). With relatively good fatigue resistance in plate forms, alloy 2024 continues in many aerospace structural applications. This datasheet provides information on composition, physical...