1-4 of 4 Search Results for

ALCOA 2036 ALLOY

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Alloy Digest (1986) 35 (5): Al-267.
Published: 01 May 1986
... ALCOA 2036 ALLOY was the first modern commercially acceptable aluminum autobody sheet alloy. It has been widely used in outer panel applications. It has moderate strength and formability and good strength after forming when no benefit can be expected from subsequent primer paint bake thermal...
Journal Articles
Alloy Digest (1989) 38 (10): Al-300.
Published: 01 October 1989
.... It is not susceptible to Luders or stretcher-strain lines. See also Alcoa 2036 Alloy, Alloy Digest Al-267, May 1986. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as fatigue. It also includes information on corrosion resistance as well as forming...
Journal Articles
Alloy Digest (1986) 35 (1): Al-264.
Published: 01 January 1986
... and/or adhesive bonded. Resistance weldingelectrode tip life is equal to or superior to Alloy 2036 and markedly superior to Alloy 5182. Corrosion Resistance: ALCOA 6010 ALLOY has high resistance inT4and T-6 tempers to 3.5 and 5 percent sodium chloride solutions in both continuous and intermittent spray exposures...
Journal Articles
Alloy Digest (1985) 34 (12): Al-262.
Published: 01 December 1985
... FOR EQUIVALENT DEEP-DENT RESISTANCE AFTER 2yc STRETCH AND PAINT BAKE I HOUR AT 350°F Alloy Relative Gage 5182 1.34 2036 1.22 6009 1.13 DDQ* Steel 1.00 *DDQ=Deep Drawing Quality. Heat Treatment: Alcoa 6009 Alloy is normally heat treated as fohows: Annealing temperature 775 F Aging temperature 350°F for 6.5 hours...