Alloy Digest (2007) 56 (5): Al-403.
Published: 01 May 2007
.... Producer or Source: Alcan Inc. Copyright © ASM International® 2007 2007 ASM International ALCAN 7449 T6511 ALCAN 7449 T79511 bearing strength chemical composition corrosion-resistant alloys elasticity fatigue properties heat treatability physical properties tensile properties...