Skip Nav Destination
Close Modal
Search Results for
ALCAN 7040-T7651
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Subjects
Journal
Article Type
Date
Availability
1-1 of 1
Search Results for ALCAN 7040-T7651
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
Sort by
Journal Articles
Alloy Digest (2008) 57 (10): Al-418.
Published: 01 October 2008
... Alcan 7040 is an Al-Mg-Zn-Cu-Zr alloy, developed to provide an improved strength-toughness balance versus incumbent 7010 and 7050 alloys. This datasheet covers Alcan 7040 alloy in T7651 temper. The alloy is used in aerospace structures. This datasheet provides information on composition, physical...
Abstract
View articletitled, <span class="search-highlight">ALCAN</span> <span class="search-highlight">7040</span>-<span class="search-highlight">T7651</span>: Al-Mg-Zn-Cu-Zr Alloy
View
PDF
for article titled, <span class="search-highlight">ALCAN</span> <span class="search-highlight">7040</span>-<span class="search-highlight">T7651</span>: Al-Mg-Zn-Cu-Zr Alloy
Alcan 7040 is an Al-Mg-Zn-Cu-Zr alloy, developed to provide an improved strength-toughness balance versus incumbent 7010 and 7050 alloys. This datasheet covers Alcan 7040 alloy in T7651 temper. The alloy is used in aerospace structures. This datasheet provides information on composition, physical properties, and tensile properties as well as fracture toughness and fatigue. It also includes information on corrosion resistance as well as forming and heat treating. Filing Code: AL-418. Producer or source: Alcan Inc.