Alloy Digest (2009) 58 (8): Al-424.
Published: 01 August 2009
... Alcan 2027 is an Al-Cu-Mg-Mn-Zr alloy, developed to provide higher strength and damage tolerance than the incumbent 2024 alloy. Alcan 2027 T3511 possesses good damage tolerance. This datasheet covers Alcan 2027 T3511 in both thin and the heavier cross sections. This datasheet provides information...