Alloy Digest (2008) 57 (9): Al-417.
Published: 01 September 2008
... This datasheet covers Alcan 2024 alloy in T3 and T351x tempers. The alloy possesses good damage tolerance. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat...
Journal Articles
Alloy Digest (2010) 59 (6): Al-429.
Published: 01 June 2010
... This datasheet covers Alcan 2024 alloy in T3 and T351x tempers for drawn tubes. The alloy possesses good damage tolerance. See also Alloy Digest Al-417, September 2008, for information about this alloy in extruded bar form. This datasheet provides information on composition, physical properties...