Skip Nav Destination
Close Modal
Search Results for
ALCAN 2024 T3
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Subjects
Journal
Article Type
Date
Availability
1-4 of 4
Search Results for ALCAN 2024 T3
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
Sort by
Journal Articles
ALCAN 2024-T3, T351X: Aluminum-Copper-Magnesium Alloy Extruded Bar
Available to Purchase
Alloy Digest (2008) 57 (9): Al-417.
Published: 01 September 2008
... This datasheet covers Alcan 2024 alloy in T3 and T351x tempers. The alloy possesses good damage tolerance. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat...
Abstract
View articletitled, <span class="search-highlight">ALCAN</span> <span class="search-highlight">2024</span>-<span class="search-highlight">T3</span>, T351X: Aluminum-Copper-Magnesium Alloy Extruded Bar
View
PDF
for article titled, <span class="search-highlight">ALCAN</span> <span class="search-highlight">2024</span>-<span class="search-highlight">T3</span>, T351X: Aluminum-Copper-Magnesium Alloy Extruded Bar
This datasheet covers Alcan 2024 alloy in T3 and T351x tempers. The alloy possesses good damage tolerance. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: AL-417. Producer or source: Alcan Inc.
Journal Articles
ALCAN 2024 T3, T351X TUBES: Aluminum-Copper- Magnesium Alloy
Available to Purchase
Alloy Digest (2010) 59 (6): Al-429.
Published: 01 June 2010
... This datasheet covers Alcan 2024 alloy in T3 and T351x tempers for drawn tubes. The alloy possesses good damage tolerance. See also Alloy Digest Al-417, September 2008, for information about this alloy in extruded bar form. This datasheet provides information on composition, physical properties...
Abstract
View articletitled, <span class="search-highlight">ALCAN</span> <span class="search-highlight">2024</span> <span class="search-highlight">T3</span>, T351X TUBES: Aluminum-Copper- Magnesium Alloy
View
PDF
for article titled, <span class="search-highlight">ALCAN</span> <span class="search-highlight">2024</span> <span class="search-highlight">T3</span>, T351X TUBES: Aluminum-Copper- Magnesium Alloy
This datasheet covers Alcan 2024 alloy in T3 and T351x tempers for drawn tubes. The alloy possesses good damage tolerance. See also Alloy Digest Al-417, September 2008, for information about this alloy in extruded bar form. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: AL-429. Producer or source: Alcan Inc., Alcan Aerospace.
Journal Articles
ALCAN 2056 T3: Aluminum Alloy Fuselage Clad Sheets
Available to Purchase
Alloy Digest (2007) 56 (6): Al-404.
Published: 01 June 2007
...: 2056 is delivered in O or T3 temper depending on customer requirements. Corrosion Resistance: The cladding consumption of 2056 clad sheet is lower than that of 2024 clad sheet (typically 3.2 mm). See Fig. 2. Specification Equivalents: AMS 4298 MMPDS pending ALCAN 2056 T3 Filing Code: Al-404 Aluminum...
Abstract
View articletitled, <span class="search-highlight">ALCAN</span> 2056 <span class="search-highlight">T3</span>: Aluminum Alloy Fuselage Clad Sheets
View
PDF
for article titled, <span class="search-highlight">ALCAN</span> 2056 <span class="search-highlight">T3</span>: Aluminum Alloy Fuselage Clad Sheets
Alcan 2056 clad alloy is an Al-Cu-Mg-Zn alloy, designed to improve assembly corrosion resistance, while exhibiting a good balance of tensile properties and high damage tolerance properties.This data sheet covers Alcan 2056 as clad sheet. Tempers are presented that show improvement over the 2024 alloy. This datasheet provides information on tensile properties as well as fatigue. It also includes information on corrosion resistance as well as forming and heat treating. Filing Code: AL-404. Producer or source: Alcan Inc.
Journal Articles
ALUMINUM 2014: Heat Treatable Aluminum Alloy
Available to Purchase
Alloy Digest (1969) 18 (3): Al-185.
Published: 01 March 1969
... recommended lo, tapping openeons. Workability: Ho, hgmg may be done berween 830650oF for blocking and ,inr\hg Ho, forming a, 300400°F may be used for 2014-T6. The loming chuac,cnstir of Al&d 2014-T3 and 2014T4 xe compamble wiul rhose of 2024-T4. Forming of Alelad 2014-T6 rrquvo rather genemus ndii. so...
Abstract
View articletitled, ALUMINUM 2014: Heat Treatable Aluminum Alloy
View
PDF
for article titled, ALUMINUM 2014: Heat Treatable Aluminum Alloy
ALUMINUM 2014 is a heat treatable alloy having high tensile and fatigue strength. It is recommended for fittings, hardware, aircraft engine components, structures, etc. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and shear strength as well as fatigue. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Al-185. Producer or source: Aluminum Company of America. Originally published as Aluminum 14S, Alloy Digest Al-17, June 1954, revised March 1969.