1-1 of 1 Search Results for

ALAR 00.12

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Alloy Digest (1956) 5 (11): Al-45.
Published: 01 November 1956
... ALAR 00.12 is a 12% silicon-aluminum casting alloy having high corrosion resistance. It is suitable for pressure-tight and thin-wall castings. This datasheet provides information on composition, physical properties, hardness, tensile properties, and shear strength as well as fracture toughness...