Journal Articles
Alloy Digest (1987) 36 (5): TS-475.
Published: 01 May 1987
... AL TECH ARAPAHO is an air-hardening or oil-hardening tool steel depending on the size, tool geometry and other desired propties. It has exceptional toughness coupled with resistance to softening at moderately high temperatures. It is used for general blanking and forming-die applications; it also...