Alloy Digest (2007) 56 (4): SS-989.
Published: 01 April 2007
... AL 332Mo alloy is an austenitic stainless steel with relatively high chromium and nickel levels for strength, and corrosion and oxidation resistance. The alloy contains a moderate addition of molybdenum for resistance to aqueous corrosion and of manganese for resistance to oxidation in air...