1-20 of 923 Search Results for

AL 20

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Alloy Digest (2005) 54 (5): SS-927.
Published: 01 May 2005
... International AL 20 chemical composition corrosion-resistant alloys elasticity hardness heat treatability joinability physical properties tensile properties thermal properties UNS N08020 Chemical Composition, wt (per ASTM B 463) Carbon 0.02 Manganese 0.40 Phosphorus 0.025 Sulfur 0.002 Silicon...
Journal Articles
Alloy Digest (1960) 9 (2): Al-89.
Published: 01 February 1960
... RED X-20 is a heat treatable hypereutectic aluminum-silicon alloy with excellent wear resistance and a very low coefficient of thermal expansion. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes information on high...
Journal Articles
Alloy Digest (1954) 3 (9): Al-20.
Published: 01 September 1954
... compressive and shear strength as well as fatigue. It also includes information on high temperature performance and corrosion resistance as well as heat treating, machining, and joining. Filing Code: Al-20. Producer or source: Aluminum Company of Canada Ltd. Producer or Source: Aluminum Company of Canada...
Journal Articles
Alloy Digest (2020) 69 (3): Al-462.
Published: 01 March 2020
...) (Btu/(h·ft·°F)) 20 °C (68 °F) 110 140 (63.6 80.9) Specific heat capacity J/(kg K) (cal/(g °C)) 100 °C (212 °F) 910 (0.217) Electrical conductivity MS/m (%IACS) 20 °C (68 °F) 16 23 (27.6 39.7) Copyright © 2020, ASM International®. All rights reserved. RAFFMETAL EN AB-AL Cu4MgTi (EN AB-21000) (Heat...
Journal Articles
Alloy Digest (2021) 70 (4): Al-475.
Published: 01 April 2021
... Raffmetal EN AB-Al Si7Mg (EN AB-42000) is a heat-treatable, aluminum-silicon-magnesium casting alloy in ingot form for remelting. It is used extensively for producing sand and permanent mold castings for applications requiring a combination of good strength and ductility, and good corrosion...
Journal Articles
Alloy Digest (2020) 69 (8): Al-467.
Published: 01 August 2020
...) (cal/(g °C)) 100 °C (212 °F) 963 (0.23) Electrical conductivity MS/m (%IACS) 19 25 (32.8 43.1) Mechanical Properties See Tables 1, 2, and 3. Table 1 Mechanical properties of sand cast EN AC-Al Si2MgTi Property Unit Value(a) Temper: F (as-cast) Tensile strength MPa (ksi) 140 (20) 0.2% proof strength...
Journal Articles
Alloy Digest (1962) 11 (6): Cu-118.
Published: 01 June 1962
... elasticity fatigue resistance fracture toughness hardness heat treatability joinability LUMEN ALLOY 20 machinability physical properties tensile properties wear resistance -DATA ON WORLD WIDE ME1 LUMEN ALLOY 20 Filing Code: G-118 Copper Alloy JUNE 1962 ALS AND ALLOYS Pnblisbed by Engineering...
Journal Articles
Alloy Digest (1971) 20 (12): SA-270.
Published: 01 December 1971
... REPUBLIC HP g-4-20 Smd-Al oy DECEMBER 1071 DIGEST a - DATA ON WORLD WIDE METALS AND ALLOYS . pauidaiby -tiDibar,ioc Upper Montclair, New Jm REPUBLIC HP 94-20 (Heat-Treated Alloy Steel; Consumable Electrode Vacuum Melted) REPUBLIC HP g-4-20 is designed especially for applications requiring optimum...
Journal Articles
Alloy Digest (2004) 53 (8): SS-906.
Published: 01 August 2004
... AL 4565 alloy has a high level of austenitizers, which provides the microstructure with a high resistance to sigma formation during welding. The high nitrogen also gives the alloy superior strength among the austenitics. Applications include flue gas desulfurization and handling seawater. This...
Journal Articles
Alloy Digest (2020) 69 (2): Al-461.
Published: 01 February 2020
... elasticity. It also includes information on joining. Filing Code: Al-461. Producer or source: Alcoa Corporation. Producer or Source: Alcoa Corporation Copyright © ASM International® 2020 2020 ASM International Alcoa EZCast 370 chemical composition physical properties elasticity joinability...
Journal Articles
Alloy Digest (2020) 69 (1): Al-460.
Published: 01 January 2020
... 4AD Tel: +44 20 7781 2000 Web: www.riotinto.com ISSN: 002-614X Al 460B Table 2 Heat treatment Temper Solution heat treatment(a)(b) Precipitation heat treatment T4 Heat to 510±5 °C (950±10 °F) and soak for 2 h. Then raise the temperature to 530±5 °C (985±10 °F) and soak for 14 20 h. Quench in water at...
Journal Articles
Alloy Digest (2021) 70 (3): Al-474.
Published: 01 March 2021
..., United Kingdom Rio Tinto Limited EN AB-Al Si6Cu4 (EN AB-45000) Tel: +44 20 7781 2000 ASTM B179:2018 ISO AB-Al Si6Cu4 Web: www.riotinto.com EN 1676:2020 AlSi6Cu4 ISO 17615:2007 All data from Primary Aluminum Foundry Alloys, Rio Tinto, JIS H 2211:2010 2019, except where noted. ISSN: 002-614X Al 474B ...
Journal Articles
Alloy Digest (1990) 39 (1): SS-511.
Published: 01 January 1990
... (Btinell) 79(150) Table 4 -GEZNERAL CORROSION OF AL 904L ALLOY AND AISI TYPE 316 STAINLESS STEEL IN VARIOUS BOILING SOLUTIONS (LABORATORY TESTS) Corrosion Rate. milshrear Boiling Solution 20% acetic acid 45% formic acid 1% hydrochloric acid 10% oxalic acid 20% phosphoric acid 10% sodium bisulfate 50...
Journal Articles
Alloy Digest (2002) 51 (5): Al-377.
Published: 01 May 2002
... information on low and high temperature performance as well as joining. Filing Code: AL-377. Producer or source: AlcoTec Wire Corporation. Producer or Source: AlcoTec Wire Corporation Copyright © ASM International® 2002 2002 ASM International ALCOTEC WELD WIRE 5554 chemical composition...
Journal Articles
Alloy Digest (2002) 51 (6): Al-378.
Published: 01 June 2002
... also includes information on corrosion resistance as well as joining. Filing Code: AL-378. Producer or source: AlcoTec Wire Corporation. Producer or Source: AlcoTec Wire Corporation Copyright © ASM International® 2002 2002 ASM International AlcoTec Weld Filler Wire 5556 aluminum brazing...
Journal Articles
Alloy Digest (2002) 51 (7): Al-379.
Published: 01 July 2002
... on corrosion resistance as well as joining. Filing Code: AL-379. Producer or source: AlcoTec Wire Corporation. Producer or Source: AlcoTec Wire Corporation Copyright © ASM International® 2002 2002 ASM International AlcoTec Weld Filler Wire 5654 chemical composition corrosion-resistant...
Journal Articles
Alloy Digest (2002) 51 (11): Al-382.
Published: 01 November 2002
... datasheet provides information on composition, physical properties, and tensile properties. It also includes information on joining. Filing Code: AL-382. Producer or source: AlcoTec Wire Corporation. Producer or Source: AlcoTec Wire Corporation Copyright © ASM International® 2002 2002 ASM...
Journal Articles
Alloy Digest (2003) 52 (1): Al-384.
Published: 01 January 2003
... also includes information on joining. Filing Code: AL-384. Producer or source: AlcoTec Wire Corporation. Producer or Source: AlcoTec Wire Corporation Copyright © ASM International® 2003 2003 ASM International Alcotec Weld filler wire 5183 brazing filler metal wire chemical composition...
Journal Articles
Alloy Digest (2002) 51 (4): Al-376.
Published: 01 April 2002
... Alcotec Weld Wire 5356 is a non-heat-treatable wire with moderate high strength capabilities. This datasheet provides information on composition, physical properties, tensile properties, and shear strength. It also includes information on joining. Filing Code: AL-376. Producer or source: AlcoTec...
Journal Articles
Alloy Digest (2005) 54 (9): SS-940.
Published: 01 September 2005
... CARPENTER 303 Al MODIFIED chemical composition corrosion-resistant alloys elasticity hardness heat treatability high-temperature alloys joinability machinability physical properties tensile properties workability UNS S30345 Chemical Composition, wt (Type analysis) Carbon 0.15 max Manganese...