Alloy Digest (2020) 69 (1): SS-1313.
Published: 01 January 2020
... AK Steel Type 201 is a chromium-manganese-nickel austenitic stainless steel that was developed to conserve nickel. Its properties are similar to those of Type 301. It is a lower cost alternative to Type 301 in certain environments. This datasheet provides information on composition, physical...
Journal Articles
Alloy Digest (2000) 49 (11): SS-809.
Published: 01 November 2000
... a weld filler is needed, AWS E/ER 308 is most often specified. Type 201 stainless steel is well known in reference lit- erature, and more information can be obtained there in. Corrosion Resistance: The general level of corrosion resistance of Type 201 is similar to that of Type 301. Type 201 should...