1-3 of 3 Search Results for

AK Steel 409 Ni

Sort by
Journal Articles
Alloy Digest (2021) 70 (6): SS-1336.
Published: 01 June 2021
... AK Steel 409 Ni is a 11% chromium ferritic stainless steel microalloyed with titanium and nickel. It provides excellent weldability, toughness, and fabricating characteristics superior to those of type 409 stainless steel in thicknesses over 3.05 mm (0.120 in.). This alloy is a cost effective...
Journal Articles
Alloy Digest (2006) 55 (3): SS-955.
Published: 01 March 2006
.... The corrosion resistance of AK Steel 41003 stainless steel is similar to other 11% Cr stainless steels such as AK Steel 409 Ni and UNS S40900. The ferritic class of stainless steels is generally considered to be weldable by the common fusion and resistance techniques. Special consideration is required...
Journal Articles
Alloy Digest (2020) 69 (1): SS-1314.
Published: 01 January 2020
... Nitrogen 0.03 Niobium (d) (e) Iron bal bal (a) Maximum values, unless indicated otherwise. (b) Types 434 and 436: 0.751.25% Mo. (c) Type 430: 0.75% Ni. (d) Type 430: 5C to 0.80% Nb. (e) 10(C+N) to 0.80% Nb. Source: AK Steel and ASTM A240/A240M:2019. Physical Properties See Table 1. Mechanical Properties...