Alloy Digest (2002) 51 (11): SS-867.
Published: 01 November 2002
... AK Steel Type 305 has the advantage of economical fabrication. Its chief characteristics are minimum work-hardening tendencies and maximum ductility. The alloy is especially suited to operations involving severe cold work such as deep drawing and spinning. It can be annealed to greater softness...
Journal Articles
Alloy Digest (1994) 43 (12): SS-577.
Published: 01 December 1994
... Stainless Steel DECEMBER1 994 - DIGEST- DATA ON WORLD WIDE METALS AND ALLOYS P&shedbyr Ak+y DQesf. Inc /x)1677-9161 21 Canliild Slreel Orurge. N.J. 070501 USA SANDVIK@ 8RElO (High temperature austenitic stainless steel) SANDVIK 8RElO is an austenitic, stainless chromium-nickel steel of the 25/20 type...