1-20 of 41 Search Results for

AISI type T15

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1968) 17 (5): TS-206.
Published: 01 May 1968
... AISI type T15 is a cobalt type high-speed steel having maximum abrasion resistance and red hardness. It is recommended for all types of cutting tools where the machining operation is different and extreme. This datasheet provides information on composition, physical properties, hardness...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1980) 29 (7): TS-365.
Published: 01 July 1980
... CPM REX 25 is a super high-speed steel made without cobalt. It is comparable to AISI Type T15 cobalt-containing high-speed steel in response to heat treatment, properties, and tool performance. CPM REX 25 is recommended for machining operations requiring heavy cuts, high speeds and feeds...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1995) 44 (4): TS-537.
Published: 01 April 1995
...#laas.AlrpvD&p6t.kAllrigMsfOWlWd. P&&hod by: Alloy Digool. Inc I201-677-9161 glpbouadti 27 C&field street. Orzqo. NJ. 07050 I U.SA THYRAPIDm PT15 ESH* (AISI T15 type high speed steel) THYRAPID PT 15 ESH is a high speed tool steel made by the rapid solidification of powder followed by Electra Slag Heating...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2007) 56 (3): TS-249.
Published: 01 March 2007
... in undesirable distortion. Specification Equivalents: AISI type T15 SAE type T15 General Characteristics: This alloy is a super-high-speed steel made by the CPM process. It is a tungsten type high-speed steel containing high vanadium for excellent abrasion resistance, and cobalt for good red hardness. This alloy...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1986) 35 (4): TS-456.
Published: 01 April 1986
... Jersey 07050 (201) 761-1090 DYNAVAN (High-Speed Steel; AISI Type T15) DYNAVAN is a DESEGATIZED* super high-speed steel containing a high percentage of both carbon and vanadium to produce an abundance of wear-resisting vanadium carbide particles. These vanadium carbides impart increased abrasion...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2010) 59 (10): TS-693.
Published: 01 October 2010
... Equivalents: AISI Type T15 SAE Type T15 General Characteristics: REX M3-1 is a lower carbon, lower vanadium modification of M3-2 high speed steel. This lower alloy content results is better machining and grinding characteristics compared to M3-2, with a slight improvement in toughness and a moderate decrease...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1977) 26 (3): SS-337.
Published: 01 March 1977
... 100 90 125 110 30-35 25-30 m/s 0.79 0.66 0.51 0.46 0.64 0.56 0.15-0.18 0.13-0.15 ipr mm/rev 0.00 l-0.003 0.03-0.08 0.002-0.004 0.05-0.10 0.00 l-0.005 0.03-0.13 0.001-0.005 0.03-0.13 0.003-0.006 0.08-0.15 0.003-0.006 0.08-O-l 5 - - Suggested Tool Material AISI Type T15 T15 T15 T15 M2 M2 Ml or hl2 Ml...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1997) 46 (1): TS-549.
Published: 01 January 1997
... as a volume loss as required by the ASTM smndard. Note, therefore, that a lower number indicates better wear t&stance. Specification Equivalents: AISI Type T15 UNS T12015 Time--Seconds (Log Scale) Fs 2 Isakml uaas-n diagnm for Caqemr MiamMdr T-15 aby. A-1260OC General Characteristics: Carpemer Micro-Melt T-15...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1976) 25 (5): TS-301.
Published: 01 May 1976
... before the weld cools below a red heat will prevent cracking at the weld. Because of its high cobalt and vanadium content, Panther 5 may crack if it is forged at too low a temperature or cooled too rapidly after the forging operation. Specification Equivalents: AISI Type T15. General Characteristics...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1979) 28 (6): SS-366.
Published: 01 June 1979
...) M2. T5, T15 Carbide Material Speed Feed Tool sfpm (m/s) ipr (mm/r) Material 165 (0.83) 0.012 (0.30) c-2 220 (1.10) 0.007 (0.18) c-3 DOI: 10.31399/asm.ad.ss0366 Copyright © ASM International® 1996 Table 4 - CORROSION DATA ON CARPENTER 18Cr-ZNi-12Mn AND AISI TYPE 304 (Annealed condition) Average...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2003) 52 (5): SS-884.
Published: 01 May 2003
.... In addi- tion, customers may be able to attain average machining speed improvements of 50% and higher over stainless AISI Type 303. This alloy has been designed to reduce tool wear and increase machine speeds and feeds to help improve productivity and reduce part costs. It is a good general purpose...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1984) 33 (10): TS-429.
Published: 01 October 1984
... HS-100 is a super high-speed steel built on an AISI Type M33 base but with higher carbon and cobalt. It is able to attain an approximate hardness of Rockwell C 68 with normal heat treatment. It gains its great resistance to wear from its high hardness rather than from excess vanadium carbides. HS...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2003) 52 (3): SS-878.
Published: 01 March 2003
... stainless is an improved-machining version of conventional Type 316/316L stainless and replaces Project 70 and Project 7000 alloys of the same grade. (See Alloy Digest SS-339 and SS-515.) Users may be able to attain machining-speed improvements of up to 50% and higher over AISI Type 316/316L. This product...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2003) 52 (4): SS-882.
Published: 01 April 2003
... to shape. Machinability: Project 70+ Type 416 stainless steel cuts very freely, primarily because of the addition of sulfur. When used in automatic screw machines, this grade machines like AISI C1117. Additional data on drilling and die threading are available from the producer. Weldability: Project 70...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2003) 52 (2): SS-875.
Published: 01 February 2003
... and Project 7000 alloys of the same grade (see Alloy Digest SS-418 and SS-513). Users may be able to attain machining speed improvements of up to 50% and high- er over AISI Type 304/304L. This material has been designed to reduce tool wear and increase machine speeds and feeds to help improve productivity...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2023) 72 (2): CS-241.
Published: 01 February 2023
... premium high speed tool steel ( S9, S10, S11, S12 or T15, M33, M41 M47 Source: Ref 47 (p 2-133) Alloy Digest: Data on Worldwide Metals and Alloys CS-241 / 10 Table 16 Recommended machining data Drilling Tool material Speed 1.5 mm (0.062 in.) 3 mm (0.125 in.) ISO (AISI or C) m/min fpm mm/rev ipr mm/rev...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2005) 54 (1): SS-915.
Published: 01 January 2005
... that is approximately 30% of AISI 1212. Slow to moderate speeds, moderate feeds, and rigid tools should be considered; tools must be kept sharp. Chips tend to be tough and stringy. Chip curlers or breakers are helpful. Use a sulfurized cutting fluid, preferably of the chlorinated type. The typical feeds and speeds...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2006) 55 (9): SS-973.
Published: 01 September 2006
...% of AISI 1212. Slow to moderate speeds, moderate feeds, and rigid tools should be considered. Chips tend to be tough and stringy. Chip curlers or breakers are helpful. Use a sulfurized cutting fluid, preferable of the chlorinated type. See Table 2. The speeds and feeds in Tables 2(a) to 2(d...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2023) 72 (2): CS-240.
Published: 01 February 2023
... and tempered. (a) Any premium high speed tool steel ( S9, S10, S11, S12 or T15, M33, M41 M47 Source: Ref 49 (p 3-7, 3-8) Table 18 Recommended machining data Reaming Tool material Speed 3 mm (0.125 in.) 6 mm (0.25 in.) ISO (AISI or C) m/ mm/ mm/ min fpm rev ipr rev ipr Treatment condition: +AR, +N, +A, or +C...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1980) 29 (2): TS-359.
Published: 01 February 1980
... FAGERSTA M-7 is a molybdenum-type high-speed steel similar to AISI Type M1, but with higher percentages of carbon and vanadium than M1. The higher levels of carbon and vanadium provide an improved cutting efficiency without significantly lowering toughness. The many applications of FAGERSTA M-7...