1-20 of 32 Search Results for

AISI type A2

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1965) 14 (8): TS-168.
Published: 01 August 1965
... AISI Type-A2 is a high-carbon, chromium, molybdenum tool and die steel having excellent non-deforming properties, abrasion resistance, toughness and good machinability. It is used for blanking and forming dies, rolls, punches, gauges, broaches, etc. This datasheet provides information...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1986) 35 (5): TS-457.
Published: 01 May 1986
... AL TECH A-HT is a tool steel for difficult cold-work applications. It is somewhat similar to AISI Type A2 in alloy content but with increased wear resistance. Additions of titanium and tungsten produce hard, long-wearing carbides that help to decrease galling and metal pick-up. The main advantages...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1974) 23 (6): TS-272.
Published: 01 June 1974
... BETHLEHEM A HT is a tool steel for cold-work applications. It is characterized by high resistance to wear, low distortion in heat treatment and air hardening; in fact, it is superior to AISI Type A2 for wearability and shock resistance. This datasheet provides information on composition, physical...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1990) 39 (6): TS-501.
Published: 01 June 1990
... TOOL STEEL Filing Code: Tool Steel TS-501 - DIGEST- DATA ON WORLD WIDE METALS AND ALLOYS JUNE 1990 eyight 1990. Al& LXgest. Inc. All rights mwvd PdMby: Alloy Oiiet, Inc. /201-677-9161 y!g No. 484* TOOL STEEL 27 CatWield Stmel. Orange. N.J. 07050 I U.S.A. (Air Hardening Tool Steel: AISI Type A2) No. 484...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1985) 34 (10): TS-448.
Published: 01 October 1985
... SELECT* 6 Alloy Digest. Inc. 27 Canfield Street Orange. New Jersey 07050 (201) 761-1090 (Cold-Work Die Steel; AISI Type A2) SELECT B is a DESEGATIZED* fully uniform air-hardening die steel having abrasion resistance intermediate between Olympic (AISI Type D2) high-carbon, high-chromium die steel...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1977) 26 (3): TS-315.
Published: 01 March 1977
... UHB RIGOR A2 wear resistance workability UHB RIGOR A2 Filing Code: TS-315 Tool Steel MARCH 1977 - DATA ON WORLD WIDE METALS AND ALLOYS UHB RIGOR+ A2 Psbiirbd by Eogineering AIIOYS Digest Inc. (Air-Hardening Cold Work Steel; AISI Type A21 Upper MontcZr, New Jw UHB RIGOR AR is a chromium-molybdenum...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1980) 29 (6): TS-364.
Published: 01 June 1980
..., expanded mica or dry lime to give a slow cooling rate which minimizes the danger of cooling cracks; this is very important. The finished hot-worked material should be annealed as soon as possible after cooling and before machining or hardening. Specification Equivalents: AISI Type A2. ME Type A2. ASTM...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1973) 22 (6): TS-257.
Published: 01 June 1973
...- ification in chemical composition in that a higher silicon content is permissible than in AISI Type A2 (wrought) tool steel. The alloy is an air-hardening alloy, intermediate in abrasion resistance between the oil- hardening and high-carbon types. It possesses good toughness characteristics along...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1978) 27 (3): TS-331.
Published: 01 March 1978
... work Sagamore below 15000F. After forging, allow the steel to cool very slowly, preferably buried in ashes, lime, expanded mica, or similar materials. Anneal as soon as possible. Specification Equivalents: AISI Type A2. SAE Type A2. UN.5 T30102. ASTM A 681 (Type A2). General Characteristics: Sagamore...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1985) 34 (2): TS-435.
Published: 01 February 1985
... Tool Steel Or FEBRUARY 1995 bIGBST - DATA ON WORLD WIDE METALS AND ALLOYS @ Copyright 1980, Enginaaring Publications, Inc. A41 rights reserved. IW: 002-614X fuhlrshed hi Alloy Digest. Inc. 27 Canfield Street Orange. New Jersey 07050 (201) 761-1090 AIRKOOL (Air-Hardening Tool Steel: AISI Type A2...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1981) 30 (11): TS-390.
Published: 01 November 1981
... to applications which require more toughness than AISI Type A2 and high-bon highchromium die steels which are actually too abrasive for convedcmal shock-resisting steels. This alloy is also recommended for specialized hot-work applica- tion where erosion, wash, and wear of the lower carbon hot- work steels...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1981) 30 (9): TS-386.
Published: 01 September 1981
... and wear resistance is essential. The mechanical properties are superior to many types of shock-resisting steels. It is particularly adapted to applications which require more toughness than AISI Type A2 and high-carbon high-chromium die steels, and are too abrasive for conventional shock-resisting steels...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1987) 36 (3): TS-472.
Published: 01 March 1987
... to produce a mechanical bond. AISI Type 308 stainless steel tiller weld metal may be used. AL Tech Apache has less carbon and chromium than AISI Type A2 and is. therefore. less wear resistant. The lower carbon and other alloying ingredients in Apache gives this steel more toughness. See Table 2 for impact...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1975) 24 (6): TS-288.
Published: 01 June 1975
... exhibited by AISI Types A2 and D2. Forms Available: Billets, bars, rods, forgings and extruded tubing. Applications: Rolling element bearings and other high-load structural com- ponents for high-temperature use, cold-work dies, cold-blanking dies, and cold-forming punches. Manufacturer: Allegheny Ludlum...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1998) 47 (11): TS-563.
Published: 01 November 1998
... tooling ecatorny than high-carbon. high-chromium steels of the D2 type (W.Nr. 2080). AISI A2 hss much better machining and grinding properties. Applications: Cutting tools for blanking, punching, piercing, cropping. shearing, trim- ming, and clipping. short cold shears. rotary shear blades for plastic...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1997) 46 (2): TS-550.
Published: 01 February 1997
...- faces. (See Alloy &?sv Ts-167. Ts-168, m-235, 75-237, and Lulcens Steel colnpany E-297 for additional infmon on these AISI type tool steels.) CoatesvilIe, PA 19320 (610) 383-2454 Products Available: Plate:A2,M.Ol.andS7areavailableto61~inthickness.S5is available to 21/4 in. thickness. ISSN: 002-614X Ts...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1965) 14 (3): TS-160.
Published: 01 March 1965
... cooled co room temperature. Specification Equivalents: Fed. QQ-T-580-A2 AISI Type A-2 SAE Type A-2 General Characteristics: No. 484FM is a very deep-hardening steel and will harden throughouc in heavy sections. Being air hardening, it holds size and shape during heat creatment. The best combination...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1968) 17 (6): TS-207.
Published: 01 June 1968
.... QQ-S-00778 Cl. FS-A2 AISI Type A-2 S.4E Type .4-2 General Characteri sti cs: Air-Hard is a high-carbon alloy tool and die steel that will not shrink or warp when cooled in still air, retains its shape, and will not crack through thin sections. It is well suited for making intricate dies, punch plates...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1965) 14 (12): TS-172.
Published: 01 December 1965
...: AISI Type A-2 SAE Type A-2 Fed. QQ-S-00778 Cl. FS-A2 General Characteristics: Airvan is a deep-hardening, air-hardening, low distortion, cough alloy cool steel with high strength and good wear resisting characteristics. Since the alloy should be cooled in air, except in extremely special cases, a minor...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1970) 19 (6): TS-231.
Published: 01 June 1970
... cooled to room temperature. *Recommended by N.E. Woldman. Specificetion Equivalents: Fed. QQSOO778Cl. FS-A2 AlSl Type A-2 SAE Type A-2 General Characteristicsz AIRKOOL-S is a high-carbon, chromium-molybdenum tool and die steel having excellent combinations of toughness, abrasion resistance...