1-5 of 5 Search Results for

AISI type 303Se

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Alloy Digest (1961) 10 (12): SS-126.
Published: 01 December 1961
... as well as forming, heat treating, machining, and joining. Filing Code: SS-126. Producer or source: Stainless steel mills. Producer or Source: Stainless steel mills Copyright ┬ę ASM International┬« 1996 1996 ASM International AISI type 303 AISI type 303Se chemical composition corrosion...
Journal Articles
Alloy Digest (1990) 39 (5): SS-512.
Published: 01 May 1990
... UNILOY 303 and 303Se are improved machinability grades of 18-8 general purpose austenitic stainless steels. Machinability is respectively improved by additions of sulfur or selenium. Whereas standard 18-8 stainless steel had a machinability rating about 40-50% that of AISI B1112 free-machining...
Journal Articles
Alloy Digest (1978) 27 (11): SS-358.
Published: 01 November 1978
.... Specification Equivalents: AL Tech 203EZ is covered by AMS 5762, ASTM A 581 and A 582. and MIL-W-52263. AL Tech 303EZ is AISI 303 and UNS No. S30300. AL Tech 303Se is AISI 303Se. Other soecitications for AL Tech 303EZ and 303Se include AMS 5640, ASTM A 581 and A 582, and MIL-W-52263. General Characteristics: AL...
Journal Articles
Alloy Digest (1975) 24 (6): SS-312.
Published: 01 June 1975
.... psi PROPERTIES Table 1 - ROOM-TEMPERATURE TENSILE PROPERTIES OF UNILOY 18-2 FM AND TWO OTHER STAINLESS STEELS Grade Tensile Yield Strength Strength (0.2% Offset) psi Psi Annealed Properties Uniloy 18-2 Fhl 70000 AISI Type 303 90000 AISI Type 416 7.5000 Cold-Drawn Properties Uniloy 18-2 FM 8.5000 AIS1...
Journal Articles
Alloy Digest (1983) 32 (9): SS-432.
Published: 01 September 1983
...-FM has excellent cold headability and machinability. It is an austenitic stainless steel and becomes only very faintly magnetic after severe cold working. It can be considered as a substitute for AISI Types 303 and 303Se. if specifications permit. (This alloy is not covered by specifications which...