Alloy Digest (1964) 13 (6): SS-156.
Published: 01 June 1964
... AISI No. 630 is a precipitation hardening stainless steel which is used in a variety of applications requiring strength combined with corrosion resistance. It is recommended for chemical process equipment, valve parts, aircraft fittings, pump shafts, etc. This datasheet provides information...
Journal Articles
Alloy Digest (2018) 67 (12): SS-1300.
Published: 01 December 2018
...; AMS 5622 UNS S17400; UNS 17400 type II ASTM A564; UNS S17400 AISI 630; ASME SA-564 General Characteristics This grade is a PH (Precipitation Hardening) martensitic stainless steel of premium quality, mainly designed for aerospace and instrumentation purposes. Overaging (aging beyond the peak strength...
Journal Articles
Alloy Digest (2007) 56 (5): TS-649.
Published: 01 May 2007
... Thyrodur 2550 is a cold-work steel with very good toughness. It is dimensionally stable, impact-resistant, and has a high hardening capacity. It is similar to AISI S1. A typical application is as cold shear knives. This datasheet provides information on composition, physical properties...
Journal Articles
Alloy Digest (1998) 47 (11): SS-732.
Published: 01 November 1998
... resistance closely approaches that of AISI types 302 and 304. Note: Under no circumstances should this alloy be used in condition A. Tests indicate that Custom 630 is highly resistant to stress corrosion cracking when heat treated at 552 C (1025 F) or higher temperatures, The higher the heat-treated...
Journal Articles
Alloy Digest (2017) 66 (12): SS-1274.
Published: 01 December 2017
... UGI 4062 is a duplex ferritic/austenitic stainless steel with good general resistance to corrosion, improved mechanical strength, and improved stress-corrosion resistance compared to AISI Type 304. This datasheet provides information on composition, physical properties, hardness, elasticity...
Journal Articles
Alloy Digest (2003) 52 (6): SS-886.
Published: 01 June 2003
... of strength, ductility, and corrosion resistance is obtained by solution treating the welded part before aging. If welding in the overaged condition, the part must be solution treated and then aged. Specification Equivalents: UNS S17400 AISI Type 630 AMS 5643 ASTM A 564 and F 899 ASME SA564 General...
Journal Articles
Alloy Digest (2018) 67 (1): SS-1275.
Published: 01 January 2018
... in the annealed condition. The machinability of this alloy is comparable to that of grade 1.4034 and significantly better than the machinability of grades 1.4112 and 1.4125 (AISI 440B/440C). Corrosion Resistance Corrosion resistance for environment and behavior is summarized below. Nitric acid Medium Phosphoric...
Journal Articles
Alloy Digest (2018) 67 (5): SS-1287.
Published: 01 May 2018
.... With a calculated average PREN of 15, this alloy has a better corrosion resistance than that of the AISI 420 series (1.4034; average calculated PREN of 13.5); but it remains less satisfactory than that of the AISI 431 series (1.4057; average calculated PREN of 17). that of the AISI 420 series (1.4034...
Journal Articles
Alloy Digest (2014) 63 (11): SS-1192.
Published: 01 November 2014
... corrosion resistance. Whereas the 209 filler metal has the best properties, grades of the AISI 308L and AISI 309 type can also be used. After welding, to achieve the best performance, a treatment in a solution at 1120 °C (2048 °F) followed by rapid cooling is recommended. Machinability: This alloy...
Journal Articles
Alloy Digest (2007) 56 (6): TS-651.
Published: 01 June 2007
... 31.0 17.9 Fig. 1 Tempering diagram See also Fig. 1 and 2. DOI: 10.31399/asm.ad.ts0651 Fig. 2 Time-temperature- transformation (TTT) diagram Specification Equivalents: AISI Type 6F7 BS M30 Werkstoff No. 1.2767 General Characteristics: Thyrodur 2767/2767 Supra has high hardenability and toughness...
Journal Articles
Alloy Digest (2007) 56 (8): TS-654.
Published: 01 August 2007
... + Bickenbach AG. Specification Equivalents: AISI Type S4 Werkstoff No. 1.2826 General Characteristics: The principal alloying elements in shock-resistant steels (S steels) are manganese, silicon, chromium, tungsten, and molybdenum, in various combinations. Carbon content is about 0.50% for all S steels, which...
Journal Articles
Alloy Digest (1954) 3 (4): SA-16.
Published: 01 April 1954
... AISI E52100 is a high-carbon, chromium alloy steel of the water hardening type. It has great depth hardenability and high wear resistance. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on forming...
Journal Articles
Alloy Digest (1997) 46 (8): TS-557.
Published: 01 August 1997
... Finkl MD AISI P-20 is an improved grade of standard AISI P-20, which is suitable for mold applications. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness. It also includes information on heat treating...
Journal Articles
Alloy Digest (1954) 3 (3): SA-15.
Published: 01 March 1954
... AISI 8640 is a nickel-chromium-molybdenum alloy steel of the oil hardening type. It has good hardenability and desirable toughness. This datasheet provides information on composition, hardness, and tensile properties as well as fracture toughness. It also includes information on low temperature...
Journal Articles
Alloy Digest (2007) 56 (12): TS-658.
Published: 01 December 2007
... be annealed before hardening to relieve any strains set up in the forging operations. Large sections (over 3 in.) should be normalized at about 845 °C (1550 °F) after forging and before annealing. Weldability: AISI type O2 is the most weldable of the oil-hardening tool steel, but welding is very difficult...
Journal Articles
Alloy Digest (2012) 61 (8): SS-1126.
Published: 01 August 2012
... the hardness. General Characteristics: This alloy is a modified AISI 420 SS and is an electro slag remelted (ESR) martensitic stainless steel developed for corrosion- resistant applications. It is supplied in the annealed condition. Table 1 Mechanical properties tensile properties (room temperature) Hardness...
Journal Articles
Alloy Digest (1954) 3 (7): SA-21.
Published: 01 July 1954
... AISI 8740 is a medium-carbon, nickel, chromium, molybdenum alloy steel of the oil hardening type. It has good hardenability and desirable toughness. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as fracture toughness. It also...
Journal Articles
Alloy Digest (2012) 61 (5): TS-702.
Published: 01 May 2012
...) use a minimum of three tempers. Average size change as a result of hardening and tempering should not exceed 0.08 mm/mm (0.003 in./in.) per maximum dimension if the tool has been stress relieved before finish machining. See Table 1 and Fig. 1. General Characteristics: Böhler K294 Microclean is an AISI...
Journal Articles
Alloy Digest (1995) 44 (5): SS-593.
Published: 01 May 1995
... Sandvik 3R60 is an austenitic stainless steel, a highly purity variant of AISI Type 316L for the urea industry. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness. It also includes information on high...
Journal Articles
Alloy Digest (1964) 13 (9): SA-167.
Published: 01 September 1964
... AISI 9260 is an oil-hardening type of spring steel and tool steel recommended for repeated and severe impact service. It is also used for heavy duty, shock resistant machine parts. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties...