1-20 of 75 Search Results for

AISI Type L6

Sort by
Journal Articles
Alloy Digest (1971) 20 (1): TS-232.
Published: 01 January 1971
... AISI Type L6 is recommended for tools, dies and machine parts which must develop a rather high degree of hardness, wear resistance and compressive strength combined with toughness. This datasheet provides information on composition, hardness, elasticity, and tensile properties. It also includes...
Journal Articles
Alloy Digest (1976) 25 (9): TS-308.
Published: 01 September 1976
... BETHALLOY* PnbIisbJ by (Low-Alloy, Special-Purpose Tool Steel; AISI Type L6) Engineering Alloys Digest, Inc Upper Moncchir, New Jersey BETHALLOY is a low-alloy oil-hardening tool steel. Because of its relatively low carbon content (for tool steels), it has slightly better shock resistance than more highly...
Journal Articles
Alloy Digest (1984) 33 (6): TS-423.
Published: 01 June 1984
.... Engineering Publications, Inc. AtI rights reserved. ISSN:OD2-614X NDS (Cold-Work Die Steel: AISI Type L6) Published b.1. Alloy Digest. inc. Post Office Box 823 Upper Montclair. New Jersey NDS is an oil-hardening steel for use in tools, dies and machine parts requiring a good combination of hardness...
Journal Articles
Alloy Digest (1981) 30 (1): TS-375.
Published: 01 January 1981
... reserved. MN: a-614X upper ~aotdair. New J-Y CYCLOPS* L6 (Special-Purpose Tool Steel; AISI Type L6) CYCLOPS L6 is an oil-hardening tool steel recommended for any tool-steel application requiring relatively great toughness, or where intricate shapes preclude the use of water-hardening steels. It is also...
Journal Articles
Alloy Digest (1959) 8 (12): TS-87.
Published: 01 December 1959
... marked hardness and brittleness in the fusion zone. Specification Equivalents: AISI Type L6 Fig? BetMeheol Allegheny Ludlum ElpaIOY e Tough No. 4 EFsE Jessop Universal-Cyclops General Characteristics: N&o-M is a chromium-nickel-molybdenum tool steel con- taining 0.70% carbon. This is a deep hardening...
Journal Articles
Alloy Digest (1983) 32 (7): TS-416.
Published: 01 July 1983
... CUTTING SPEEDS, sfpm Feed Depth of High-Speed Carbide- in. /rev. Cut, in. Steel Tipped 0.015 l/32 90 350 a015 l/l6 75 295 aoi5 118 60 250 a030 l/32 65 260 0.030 l/l6 55 215 0.030 11 3 45 180 Workabllity: AISI Type L2 should be heated slowly and uniformly for forging and other hot-working operations. Soak...
Journal Articles
Alloy Digest (1978) 27 (7): TS-335.
Published: 01 July 1978
... properties workability All Filing Code: TS-335 CYCLOPS MI Tool Steel Or JULY 1978 DIGIST - DATA ON WORLD WIDI METALS AND ALLOYS -?tiizz2%Ir CYCLOPS* M4 Uppw Many, NW Jermy (HighSpeed Tool Steel; AISI Type M4) CYCLOPS hi4 is a deep-hardening steel that was developed to utilize the excellent abrasion...
Journal Articles
Alloy Digest (1958) 7 (6): TS-71.
Published: 01 June 1958
...-Nickel Tool Steel, Type L6) CYQ.OPS N-9 is a chromium-nickel oil hardening steel with high toughness and fatigue resistance. Composition: Carbon Manganese Silicon Chromium Nickel Iron Nominal 0.75 0.40 0.25 1.00 1.50 Remainder Physical Constants: Specific gravity Density, lb./cu in Thermal coef expansion...
Journal Articles
Alloy Digest (1977) 26 (10): TS-325.
Published: 01 October 1977
... are recommended. After welding, sections should be normal- ized as given in the instructions under Normalizing and then hardened and tempered to the desired hardness. Specification Equivalents: AISI Type L2. AISI 6150 and WE 6150 (Equivalent only in composi- tion, not in mill practice). General Characteristics...
Journal Articles
Alloy Digest (1984) 33 (2): SA-397.
Published: 01 February 1984
... AISI 4161 is a low-alloy steel of the chromium-molybdenum type; it contains nominally 0.61% carbon. It has relatively high hardenability and good resistance to abrasion, impact and fatigue. It is an oil-hardening grade and is recommended for moderately heavy-duty service. This steel has...
Journal Articles
Alloy Digest (1972) 21 (11): TS-247.
Published: 01 November 1972
... AISI Type M30 is a high-speed tool steel containing 8% molybdenum and 5% cobalt. It provides long life in machining difficult-to-cut metals, such as heat-resisting alloys and superalloys, and is recommended for cutting tools requiring a good combination of suitable toughness with optimum cutting...
Journal Articles
Alloy Digest (1982) 31 (12): TS-408.
Published: 01 December 1982
... AISI Type S2 is a water-hardening tool steel with extreme toughness and resistance to shock loading. Even at a hardness of Rockwell C 59-60, it will bend before it breaks. When hardened in medium-size and large-size pieces, it acquires a hard case and a tough core. Sizes under 3/4-inch (19mm...
Journal Articles
Alloy Digest (1977) 26 (12): TS-328.
Published: 01 December 1977
...~ he. (Shock-Resisting Tool Steel; AISI Type S2) Upper Montclair, New Jersey CYCLOPS S2 is a high-silicon, shock-resisting tool steel with extreme toughness. It has good ductility and toughness at high strength levels, and gives excellent service in those applications where shock and impact are major...
Journal Articles
Alloy Digest (1974) 23 (2): TS-267.
Published: 01 February 1974
... side cuttingedge angle, and a nose radius of 1132 to l/l6 inch. Workability: AISI Type W2 can be forged by heating slowly, uniformly and thoroughly to 1800 to 1950oF. Forging should be completed at about 1500oF to insure fine austenitic grams and to leave the steel in good condition for annealing...
Journal Articles
Alloy Digest (1981) 30 (6): SS-387.
Published: 01 June 1981
... CRUCIBLE 303 PLUS-X is a non-hardenable austenitic chromium-nickel steel to which elements have been added to improve machinability and non-galling characteristics. Better machinability than that of standard AISI Type 303 stainless is obtained by the use of higher manganese content to give...
Journal Articles
Alloy Digest (1982) 31 (8): TS-402.
Published: 01 August 1982
... AISI Type M33 is a heavy-duty high-speed steel; it contains 8.00% cobalt to improved red hardness. It is recommended for cutting-tool applications in which wear resistance and high temperature hardness are important characteristics. It should not be used where excessive shock and/or chatter...
Journal Articles
Alloy Digest (1958) 7 (7): SA-71.
Published: 01 July 1958
... AISI 5140 is a low chromium alloy steel of the deep hardening type. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on forming, heat treating, machining, and joining. Filing Code: SA-71. Producer...
Journal Articles
Alloy Digest (1980) 29 (12): SS-378.
Published: 01 December 1980
... CRUCIBLE 316 PLUS is a non-hardenable austenitic chromium-nickel steel with superior corrosion and heat resisting qualities. Better machinability than that of standard AISI Type 316 stainless is obtained by the use of balanced chemistry and special manufacturing techniques. This grade is non...
Journal Articles
Alloy Digest (1975) 24 (2): SS-305.
Published: 01 February 1975
... USS 18-8S (AISI Type 304) and USS 18-8I (AISI Type 304L) are austenitic chromium-nickel steels that are easy to fabricate and weld. They combine high strength with excellent stability and shock resistance, even at cryogenic temperatures. This datasheet provides information on composition, physical...
Journal Articles
Alloy Digest (1982) 31 (10): SA-386.
Published: 01 October 1982
... or water, temper to desired hardness. Sub-Critical Anneal: Heat to llOO-1200┬░F. air cool. Machinability: The machinability rating for most machining opera- tions on annealed-and-cold-drawn SAE 50B50 steel is about 60% of AISI B1112 Bessemer screw stock. Cold-drawn hot-rolled material is only about 52...