1-9 of 9 Search Results for

AISI Type 502

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Alloy Digest (1968) 17 (7): SS-211.
Published: 01 July 1968
... AISI Type 502 is a corrosion and heat resisting 5% chromium alloy steel. It is generally used in the annealed condition only. It is recommended for oil refinery and chemical plant equipment, oil pump impellers, etc. This datasheet provides information on composition, physical properties, hardness...
Journal Articles
Alloy Digest (1989) 38 (1): SS-502.
Published: 01 January 1989
... JESSOPTYPE 317L and 317L Plus are low-carbon austenitic stainless steels with somewhat higher alloy content than AISI type 316L. This gives them superior corrosion resistance in difficult environments as well as higher elevated temperature strength characteristics. This datasheet provides...
Journal Articles
Alloy Digest (1990) 39 (10): TS-502.
Published: 01 October 1990
...: AISI T-5 General Characterlstlcs: Circle C exhibits high red hardness and excellent wear resistance. Its high degree of red hardness permits it to cut at greater speeds and feeds than most types of high-speed steels. On tools not to be ground after hardening, precau- tion must be taken to prevent...
Journal Articles
Alloy Digest (2018) 67 (9): SS-1294.
Published: 01 September 2018
... Electralloy Nitronic 32 was created to match AISI Type 304 Stainless Steel in corrosion with twice the yield strength. This datasheet provides information on composition, physical properties, and tensile properties. It also includes information on corrosion resistance as well as joining. Filing...
Journal Articles
Alloy Digest (1961) 10 (7): SS-119.
Published: 01 July 1961
... AISI Type 501 is a low-chromium type corrosion steel that is used for its heat resistance and good mechanical properties at elevated temperatures as well as for its corrosion resistance at moderately elevated temperatures. This datasheet provides information on composition, physical properties...
Journal Articles
Alloy Digest (1954) 3 (12): SS-22.
Published: 01 December 1954
... alkaline solutions, good resistsnce to oil refinery audes below 400°F., good resistance m mineral and vegetable oils, pwr resistance m am- monium and hot sulphite liquors. Specification Equivalentsz ASTM Al99, Al.0 ASTM A200, Al.8 ASTM A213, T5 ASTM Al58, P5a ASTM A132, F5 ASTM A193, B5 AISI Type 501 + MO...
Journal Articles
Alloy Digest (2002) 51 (6): SS-786.
Published: 01 June 2002
... Allegheny Ludlum alloy 255 is a high-strength duplex stainless steel. It combines high mechanical strength, ductility, and hardness with excellent resistance to corrosion and erosion. Under most conditions of service, its corrosion resistance is superior to that of the fully austenitic AISI type...
Journal Articles
Alloy Digest (1959) 8 (12): SS-98.
Published: 01 December 1959
... it is somewhat similar in composition w AISI Type 330 stainless steel, it is produced w a much higher, more uniform standard of quality than is found in the ordinary heat-resistant mechanical purpose alloy. In addition, Chromel-D also possesses certain properties which make It particularly suitable for use...
Journal Articles
Alloy Digest (2023) 72 (2): CS-240.
Published: 01 February 2023
... of non-alloy steels at various locations Location Norman Wells, NWT, Canada Phoenix, AZ, USA Potter County, PA, USA Montreal, QC, Canada Bethlehem, PA, USA Kure Beach, NC, USA(b) Kure Beach, NC, USA(c) Type of environment Polar Rural arid Rural Urban Industrial Marine Marine Average corrosion rate(a) µm...