Alloy Digest (1961) 10 (7): SS-119.
Published: 01 July 1961
... AISI Type 501 is a low-chromium type corrosion steel that is used for its heat resistance and good mechanical properties at elevated temperatures as well as for its corrosion resistance at moderately elevated temperatures. This datasheet provides information on composition, physical properties...
Journal Articles
Alloy Digest (1954) 3 (12): SS-22.
Published: 01 December 1954
... alkaline solutions, good resistsnce to oil refinery audes below 400┬░F., good resistance m mineral and vegetable oils, pwr resistance m am- monium and hot sulphite liquors. Specification Equivalentsz ASTM Al99, Al.0 ASTM A200, Al.8 ASTM A213, T5 ASTM Al58, P5a ASTM A132, F5 ASTM A193, B5 AISI Type 501 + MO...
Journal Articles
Alloy Digest (1990) 39 (6): TS-501.
Published: 01 June 1990
... TOOL STEEL Filing Code: Tool Steel TS-501 - DIGEST- DATA ON WORLD WIDE METALS AND ALLOYS JUNE 1990 eyight 1990. Al& LXgest. Inc. All rights mwvd PdMby: Alloy Oiiet, Inc. /201-677-9161 y!g No. 484* TOOL STEEL 27 CatWield Stmel. Orange. N.J. 07050 I U.S.A. (Air Hardening Tool Steel: AISI Type A2) No. 484...
Journal Articles
Alloy Digest (1987) 36 (6): Ni-349.
Published: 01 June 1987
...-strength uses Excellent Variable dimensions and wide gaps Not recommended *Depends on design of brazements. base metal and brazing condition. Table 2 - BRAZED JOINT HARDNESS (AISI Type 316 stainless steel base metal) Knoop microhardness 266 r 8 ( IOO-gram load and I-5-second indentation time.) Heat...
Journal Articles
Alloy Digest (1971) 20 (7): TS-236.
Published: 01 July 1971
... AISI Type H21 is a tungsten-chromium hot-work tool and die steel having good red-hardness and resistance to abrasion with relatively good shock resistance. It will withstand high operating temperatures up to 1000 F for long periods of time. This datasheet provides information on composition...
Journal Articles
Alloy Digest (1966) 15 (9): SS-186.
Published: 01 September 1966
... better corrosion resistance than AISI 316 or 317 steels in sulfuric acid solutions in which its utilization domain is markedly larger, as shown by the graph. In ocher solutions, its resistance is identical to that of 316 or 317 steels: sulphurous acid, sulphite liquors, sodium and calcium brines...
Journal Articles
Alloy Digest (1972) 21 (9): SA-280.
Published: 01 September 1972
...-lb** At O+ 3oF 60?L&T - 60L&T 50L&T 607 L&T 60L&T 60 60 *Forgings: properties are longitudinal for plate types and tangential for ring types. Also, see ASTM A 579, Grade 12. **The average ftdb at room temperature (70oF min) shall not exceed by more than 10 ft-lb the average at OOF. ? For Hand 9/16...