Journal Articles
Alloy Digest (1968) 17 (10): SS-215.
Published: 01 October 1968
... AISI Type 440A is a martensitic hardenable high-carbon high chromium stainless steel recommended for cutlery, valve parts, surgical instruments, etc. It is always used in the hardened condition. This datasheet provides information on composition, physical properties, hardness, elasticity...
Journal Articles
Alloy Digest (1955) 4 (12): SS-38.
Published: 01 December 1955
... to relief of residual stresses. Do not pickle hardened material without first stress- relieving. Specification Equivalents: SAE 51440A AMS 7445 Opt.1 ASTM A276 Type 440A ASTM A314 Type 440A AISI 440A General Characteristics: This steel is always used in the hardened condition; and after heat treatment...
Journal Articles
Alloy Digest (1984) 33 (10): SS-452.
Published: 01 October 1984
...). Specification Equivalents: AISI Type 440A. AMS 5631. ASTM: A 276, A 314, A 473, A 5 I 1 and A 580. Federal QQ-S-763. Military MIL-S-862. SAE 5405. UNS No. S44002. General Characteristics: Carpenter Stainless Type 440A is a hardenable (martensitic), chromium stainless steel. It was designed to provide stainless...
Journal Articles
Alloy Digest (1975) 24 (6): SS-312.
Published: 01 June 1975
.... psi PROPERTIES Table 1 - ROOM-TEMPERATURE TENSILE PROPERTIES OF UNILOY 18-2 FM AND TWO OTHER STAINLESS STEELS Grade Tensile Yield Strength Strength (0.2% Offset) psi Psi Annealed Properties Uniloy 18-2 Fhl 70000 AISI Type 303 90000 AISI Type 416 7.5000 Cold-Drawn Properties Uniloy 18-2 FM 8.5000 AIS1...